Advanced Photonics, Volume. 4, Issue 1, 016001(2022)
Label-free fiber nanograting sensor for real-time in situ early monitoring of cellular apoptosis
Fig. 1. Schematic illustration and design of the fiber nanogratings sensor. (a) Schematic diagram of the ZnO nanogratings integrated on a fiber bioprobe. (b) SEM image of the fiber sensor, with a nanowire diameter of 800 nm. Scale bar,
Fig. 2. Optical characteristics and RI sensitivity of the nanosensor. (a) Reflectance spectra of the fiber probe with (blue line) and without (black line) ZnO nanogratings. The peak wavelength is 658 nm. (b) Color map of spectra with different external RIs. (c) Shift in the peak reflection wavelength (black line) and the change in power at 655 nm (red line) as a function of the external RI. The red line is derived from the values in (b). (d) Dynamic response of the reflection power at 655 nm with the addition of ethanol (black line) and the power at 655 nm as a function of the external RI (red line). The figure closely coincides with the red line in (c).
Fig. 3. Intracellular calibration and measurements of the nanosensor. (a) Schematic diagram of the experimental setup used to calibrate the RI sensitivity of the probe and measure the intracellular RI of HeLa cells. A low-power laser at 655 nm (
Fig. 4. Real-time long-term early monitoring of HeLa cell apoptosis. Microscope images of single tested HeLa cells (yellow dashed circle) and other reference cells during the apoptosis process. (a) Immediately after the addition of
|
|
Get Citation
Copy Citation Text
Danran Li, Nina Wang, Tianyang Zhang, Guangxing Wu, Yifeng Xiong, Qianqian Du, Yunfei Tian, Weiwei Zhao, Jiandong Ye, Shulin Gu, Yanqing Lu, Dechen Jiang, Fei Xu, "Label-free fiber nanograting sensor for real-time in situ early monitoring of cellular apoptosis," Adv. Photon. 4, 016001 (2022)
Category: Research Articles
Received: Oct. 26, 2021
Accepted: Dec. 14, 2021
Published Online: Jan. 10, 2022
The Author Email: Jiang Dechen (dechenjiang@nju.edu.cn), Xu Fei (feixu@nju.edu.cn)