Journal of Infrared and Millimeter Waves, Volume. 43, Issue 1, 63(2024)
Correlation between MBE deoxidation conditions and InGaAs/InP APD performance
Fig. 1. Profile diagram and internal electric field distribution of InGaAs/InP APD structure
Fig. 4. (a) Comparison of SIMS depth distributions for Samples via As4, P2 deoxidation,(b) Bulk regions (d = 4.8-5.6 μm) of comparison of deoxidation interface
Fig. 5. STEM-HAADF image of APD sample A(As-deoxidation)(a)an image of the APD structure on FIB grid,(b)the image of InGaAs and InP buffer,(c)zoom region of InP homojunction interfaces,(d)high-resolution images of the region marked with a red frame in(a)
Fig. 6. STEM-HAADF image of APD sample B(P-deoxidation)(a)an image of the APD structure on the FIB grid,(b)the image of InGaAs and InP buffer,(c)the zoom region of InP homojunction interfaces and stacking fault(circled). Circles indicate dislocations with different core structures,(d)high-resolution images of the area marked with a red frame in(a)
Fig. 7. (a) I-V and gain characteristics of the InGaAs/InP APD,(b) TRPL spectra of ARC-APD
|
Get Citation
Copy Citation Text
Zi-Lu GUO, Wen-Juan WANG, Hui-Dan QU, Liu--Yan FAN, Yi-Cheng ZHU, Ya-Jie WANG, Chang-Lin ZHENG, Xing-Jun WANG, Ping-Ping CHEN, Wei LU. Correlation between MBE deoxidation conditions and InGaAs/InP APD performance[J]. Journal of Infrared and Millimeter Waves, 2024, 43(1): 63
Category: Research Articles
Received: May. 5, 2023
Accepted: --
Published Online: Dec. 26, 2023
The Author Email: WANG Wen-Juan (wangwj@mail.sitp.ac.cn), CHEN Ping-Ping (ppchen@mail.sitp.ac.cn), LU Wei (luwei@mail.sitp.ac.cn)