Chinese Journal of Lasers, Volume. 43, Issue 3, 303006(2016)
Research on Corrosion Resistanceand Wear Resistance of Laser Cladding Cr3Si/γ Multi-Phase Coating
[1] [1] Sun Rong. Study on Cathodic Oxygen Reduction Reaction at Steel in Seawater[D]. Chongqing: Dissertation of Chongqing University, 2007.
[2] [2] Li Xiaogang, Dong Chaofang, Gao Jin, et al.. The scientific research and data-sharing network of steels atmosphere corrosion in China [J]. Metal World, 2010, 4: 1-8.
[3] [3] Wei Minxian. Oxidation Wear and Mild-to-Severe Wear Transition of Ferrous Alloy under Severe Condition[D]. Jiangsu: Jiangsu University, 2011.
[4] [4] Zhang Yongzhen, Zhu Jun, Liu Weimin, et al.. Investigation of topographical characteristics and tribological behavior of compacted graphite iron in sliding against 40Cr steel under different dry sliding conditions[J]. Tribology, 2001, 21(1): 37-41.
[5] [5] Liu Shunhong. Laser Materials Processing[M]. Wuhan: Huazhong University of Science and Technology Press, 2011.
[7] [7] Feng Shurong, Zhang Shuquan, Wang Huaming. Wear resistance of laser clad hard particles reinforce intermetallic composite coating on TA15 alloy[J]. Chinese J Lasers, 2012, 39(2): 0203002.
[8] [8] He Xiangming, Liu Xiubo, Yang Maosheng, et al.. Elevated temperature tribological behaviors of laser cladding nickel-based composite coating on austenitic stainless steel[J]. Chinese J Lasers, 2011, 38(9): 0903007.
[10] [10] Liu Xiaopeng, Zhang Peilei, Lu Yunlong, et al.. Study on tribological properties of Ni-based silicide coating on copper by laser cladding [J]. Chinese J Lasers, 2015, 42(9): 0906005.
[11] [11] Li Min, Huang Jian, Zhu Yanyan, et al.. Effect of BN content on microstructure evolution and wear property of in situ Ti /(TiB+TiN) hybrid composite coating by laser cladding[J]. Chinese J Lasers, 2015, 42(9): 0903001.
[12] [12] Tang H B, Fang Y L, Wang H M. Microstructure and dry sliding wear resistance of a Cr13Ni5Si2 ternary metal silicide alloy[J]. Acta Materialia, 2004, 52(7): 1773-1783.
[13] [13] Cruse T A, Newkirk J W. Evaluation of methods to produce tough Cr3Si based composites[J]. Materials Science and Engineering: A, 1997, 239-240: 410-418.
[14] [14] Zhang Liqiang, Wang Huaming. Microstructure and high-temperature sliding wear resistance of a Cr3Si/Crl3Ni5Si2 intermetallic alloy [J]. Rare Metal Materials and Engineering, 2004, 33(5): 512-514.
[16] [16] Wang H M, Duan G. Wear and corrosion behavior of laser clad Cr3Si reinforced intermetallic composite coatings[J]. Intermetallics, 2003, 11(8): 755-762.
[17] [17] Jian Lina, Zhang Lingyun, Yu Rongli, et al.. Microstructure and wear resistance of laser clad Cr13Ni5Si2-based metal silicide coating on titanium alloy[J]. Rare Metal Materials and Engineering, 2005, 34(6): 936-939.
[19] [19] Yuan L, Wang H M. Corrosion behaviors of a γ-toughened Cr13Ni5Si2/Cr3Ni5Si2 multi-phase ternary metal silicide alloy in NaCl solution [J]. Electrochimica Acta, 2008, 54(2): 421-429.
[20] [20] Gray J J, Orme C A. Electrochemical impedance spectroscopy study of the passive films of alloy 22 in low pH nitrate and chloride environments[J]. Electrochimica Acta, 2007, 52(7): 2370-2375.
[21] [21] Kocijan A, Donik C , Jenko M. Electrochemical and XPS studies of the passive film formed on stainless steels in borate buffer and chloride solutions[J]. Corrosion Science, 2007, 49(5): 2083-2098.
[22] [22] Wu Y, Wang A H, Zhang Z, et al.. Wear resistance of in situ synthesized titanium compound coatings produced by laser alloying technique [J]. Surface and Coatings Technology, 2014, 258: 711-715.
Get Citation
Copy Citation Text
Xu Jintao, Li An, Liu Dong, Wang Huaming. Research on Corrosion Resistanceand Wear Resistance of Laser Cladding Cr3Si/γ Multi-Phase Coating[J]. Chinese Journal of Lasers, 2016, 43(3): 303006
Category: laser manufacturing
Received: Oct. 21, 2015
Accepted: --
Published Online: Mar. 4, 2016