Chinese Journal of Lasers, Volume. 40, Issue s1, 103010(2013)
Laser Surface Modification of Indefinite Chilled Cast-Iron Roller
[1] [1] Yao Chengwu, Huang Jian. Application status of laser hardening and repairing technology on roller surface[J]. Material & Heat Treatment, 2007, 36(8): 69-77.
[2] [2] Zang Chenfeng, Liu Changsheng. Research progress of laser modification techniques used on roller surface[J]. Materials Review (Review Article), 2010, 24(2): 6-10.
[3] [3] Sun Guifang, Liu Changsheng, Tao Xingqi, et al.. Research on laser alloying of high-Ni-Cr infinite chilled cast iron roller[J]. Journal of Northeastern University (Natural Science), 2008, 29(6): 845-848.
[4] [4] Lu Jian, Luo Fang. Research on improving roller life by laser alloying technique[J]. Zhejiang Metallurgy, 2007, (4): 41-45.
[7] [7] Hou Xinyun, Wei Guo. The application of laser roller strengthens technology[J]. Henan Metallurgy, 2007, 15(5): 46-47.
[8] [8] Song Yang, Zhu Shigen, Qu bin, et al.. Methods to repair and strengthen surface of the roll[J]. Machinery Design & Manufacture, 2005, 8: 113-115.
[9] [9] Tong Xin, Li Fuhai, Liu Min, et al.. Thermal fatigue resistance of non-smooth cast iron treated by laser cladding with different self-fluxing alloys[J]. Optics and Laser Technology, 2010, 42(7): 1154-1161.
[10] [10] Zhang Guodong, Huang Anguo, Li Zhiyuan, et al.. Laser transformation hardening of high-Ni-Cr infinite chilled cast iron roller[A]. The Sixth National Conference on Surface Engineering[C]. 2006.
[11] [11] Li Zhaohui. Practice to strengthen surface of roller with laser[J]. Hebei Metallurgy, 2008, (2): 29-30.
[12] [12] Lin Chaowen, Wang Yong, Zhang Zhe, et al.. Influence of overlapping ratio on hardness and residual stress distributions in multi-track laser surface melting roller steel[J]. Optics and Lasers in Engineering, 2010, 48(12): 1224-1230.
[13] [13] Wu Guosheng, Wang Yutao. Laser surface hardening of high NiCr indefinite chill cast iron roll material[J]. Journal of Wuhan Engineering Institute, 2008, 20(4): 1-3.
[14] [14] YB4052-1991, Metallographic test of high-Ni-Cr infinite chilled centrifugal cast iron roller[S]. 1991.
[15] [15] Shi shihong. Influences of technology and powder in laser cladding treatment on cracking behavior of cladding layer[D]. Changsha: Central South University, 1998.
[16] [16] Dong Xiuhua. Effect of parameters of laser intensify treatment process on milling roll surface properties[J]. Journal of Baotou University of Iron and Steel Technology, 2003, 22(3): 242-246.
[17] [17] Yungchun Lee, Chengyu Chiu. Roller-based laser-assisted direct imprinting for large-area and continuous nano-fabrication[J]. Microelectronic Engineering, 2010, 87: 35-40.
[18] [18] Janne Nurminen, Jonne Nakki, Petri Vuoristo. Mcrostructure and properties of hard and wear resistant MMC coatings eposited by laser cladding[J]. Int J Refractory Metals & Hard Materials, 2009, 27: 472-478.
Get Citation
Copy Citation Text
Chen Changjun, Zhang Min, Wang Xiaonan, Zhang Chao, Jing Hemin. Laser Surface Modification of Indefinite Chilled Cast-Iron Roller[J]. Chinese Journal of Lasers, 2013, 40(s1): 103010
Category: laser manufacturing
Received: Jul. 21, 2013
Accepted: --
Published Online: Dec. 26, 2013
The Author Email: Changjun Chen (chjchen2001@aliyun.com)