Chinese Journal of Lasers, Volume. 46, Issue 3, 0302004(2019)
Forming Limit and Fracture Mode in Multiple-Pulse Laser Shock Micro-Bulging Process
Fig. 1. Schematic of experimental set-up for multiple-pulse laser shock micro-bulging process
Fig. 6. Tensile fracture morphology of T2 pure copper foil. (a) General view of fractured specimen; (b) fracture surface of region 1 after magnification
Fig. 7. Shear fracture morphology of T2 pure copper foil. (a) General view of fractured specimen; (b) enlarged fracture surface
Fig. 10. Spallation morphology of T2 pure copper foil. (a) General view of spallation fractured specimen; (b) fracture surface of region 1 after magnification
|
|
Get Citation
Copy Citation Text
Zheng Liu, Chao Zheng, Libin Song, Zhong Ji. Forming Limit and Fracture Mode in Multiple-Pulse Laser Shock Micro-Bulging Process[J]. Chinese Journal of Lasers, 2019, 46(3): 0302004
Category: laser manufacturing
Received: Jul. 30, 2018
Accepted: Dec. 4, 2018
Published Online: May. 9, 2019