Laser & Optoelectronics Progress, Volume. 55, Issue 4, 041405(2018)
Influence of Process Parameters on Forming Defects of H13 Steel Processed by Selective Laser Melting
Fig. 1. Single-channel morphologies under different laser powers. (a) 250 W; (b) 300 W; (c) 350 W; (d) 400 W; (e) 450 W
Fig. 2. Single-channel morphologies under different scanning speeds. (a) 800 mm?s-1; (b) 1000 mm?s-1; (c) 1200 mm?s-1; (d) 1400 mm?s-1; (e) 1600 mm?s-1
Fig. 3. Effect of laser power on forming part quality.(a) 250 W; (b) 350 W; (c) 400 W; (d) 450 W
Fig. 4. Effect of scanning speed on forming part quality. (a) 300 mm?s-1; (b) 400 mm?s-1; (c) 500 mm?s-1; (d) 800 mm?s-1; (e) 1200 mm?s-1
Fig. 5. Effect of scanning spacing on forming part quality. (a) 40 μm; (b) 60 μm; (c) 70 μm; (d) 80 μm
Fig. 6. Schematic of SLM scanning strategy. (a) Single X direction scanning; (b) Z-shaped orthogonal scanning; (c) S-shaped orthogonal scanning
Fig. 7. Forming quality under different scanning modes. (a) S-shaped orthogonal scanning; (b) Z-shaped orthogonal scanning; (c) single X direction scanning
|
|
|
Get Citation
Copy Citation Text
Jingang Xu, Yong Chen, Hui Chen, Bing Yang. Influence of Process Parameters on Forming Defects of H13 Steel Processed by Selective Laser Melting[J]. Laser & Optoelectronics Progress, 2018, 55(4): 041405
Category: Lasers and Laser Optics
Received: Oct. 18, 2017
Accepted: --
Published Online: Sep. 11, 2018