Acta Optica Sinica, Volume. 37, Issue 12, 1214002(2017)

Removal of Cable Shield Material by YAG Laser

Tianyu Chen, Mingdi Wang*, Guilin Yang, Kai Liu, and Keming Shi
Author Affiliations
  • School of Mechanical and Electric Engineering, Soochow University, Suzhou, Jiangsu 215021, China
  • show less
    Figures & Tables(12)
    Model of laser peeling of metallic materials
    Cloud pictures of temperature field in shielding layer. (a) Temperature field in quasi-steady state; (b) longitudinal distribution of temperature field
    Influence of laser power on peeling quality of shielding layer
    Influence of laser scanning speed on peeling quality of shielding layer
    Influence of laser frequency on peeling quality of shielding layer
    Influence of defocusing distance on peeling quality of shielding layer
    (a) Effect picture and (b) kerf surface of laser peeling of shielding layers after laser parameter optimization
    • Table 1. Process parameters and test results for laser peeling of shielding layers

      View table

      Table 1. Process parameters and test results for laser peeling of shielding layers

      Serial numberPower /WScanning speed /(mm·s-1)Frequency /kHzDefocusing distance /mmKerf width /(10-2 mm)Kerf depth /mm
      11253000.2070.019
      21453000.3610.079
      31653000.4820.120
      41853000.5160.120
      52053000.8260.120
      61613000.8610.120
      71633000.7230.120
      81673000.4310.090
      91693000.2580.062
      101651000.3270.099
      111652000.4480.120
      121654000.5610.120
      131655000.5340.109
      1416530-20.1720.040
      1516530-10.3340.087
      161653010.4290.051
      171653020.0860.006
    • Table 2. Factor level table

      View table

      Table 2. Factor level table

      LevelFactor
      A /WB /(mm·s-1)C /kHzD /mm
      115420-0.5
      2175300
      3196400.5
    • Table 3. Arrangement of orthogonal test elements and results

      View table

      Table 3. Arrangement of orthogonal test elements and results

      Serial numberElementResult
      A /WB /(mm·s-1)C /kHzD /mmKerf width /(10-2 mm)Kerf depth /mm
      115420-0.50.6860.096
      21553000.5490.120
      3156400.50.4810.104
      4174300.50.6580.112
      517540-0.50.5620.120
      61762000.4390.120
      71944000.7130.120
      8195200.50.6990.120
      919630-0.50.6720.120
    • Table 4. Range analysis results of kerf widths

      View table

      Table 4. Range analysis results of kerf widths

      FactorKerf widthR /(10-2 mm)
      k1 /(10-2 mm)k2 /(10-2 mm)k3 /(10-2 mm)
      A0.5720.5530.6950.142
      B0.6860.6030.5310.155
      C0.6080.6260.5850.041
      D0.6400.5670.6130.073
    • Table 5. Range analysis results of kerf depths

      View table

      Table 5. Range analysis results of kerf depths

      FactorKerf depthR /mm
      s1 /mms2 /mms3 /mm
      A0.1070.1170.1200.013
      B0.1090.1200.1150.011
      C0.1120.1170.1150.005
      D0.1120.1200.1120.008
    Tools

    Get Citation

    Copy Citation Text

    Tianyu Chen, Mingdi Wang, Guilin Yang, Kai Liu, Keming Shi. Removal of Cable Shield Material by YAG Laser[J]. Acta Optica Sinica, 2017, 37(12): 1214002

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: Lasers and Laser Optics

    Received: Jul. 10, 2017

    Accepted: --

    Published Online: Sep. 6, 2018

    The Author Email: Wang Mingdi (wangmingdi@suda.edu.cn)

    DOI:10.3788/AOS201737.1214002

    Topics