Laser & Optoelectronics Progress, Volume. 61, Issue 17, 1714008(2024)

Long-Pulse Output Characteristics of Solid-State Fe2+∶ZnSe Laser at Low Temperature

Hao Liu1,2, Kenan Wu1、*, and Yuqi Jin1、**
Author Affiliations
  • 1Key Laboratory of Chemical Lasers, Dalian Institute of Chemical Physics, Chinese Academy of Sciences, Dalian 116023, Liaoning, China
  • 2University of Chinese Academy of Sciences, Beijing 100049, China
  • show less
    Figures & Tables(6)
    Experimental setup of the Fe2+∶ZnSe laser
    Time-domain characteristics of pump pulse and output pulse of Fe2+∶ZnSe laser. (a) Complete pulse waveform; (b) early stage waveform
    Variation of output energy of coated Fe2+∶ZnSe crystals with pump light energy with different OCs.(a) Crystal thickness is 3 mm; (b) crystal thickness is 6 mm
    Output characteristics of uncoated Fe2+∶ZnSe crystal. (a) Laser energy with different OCs; (b) variation of laser energy with pump energy when the crystal tilted by 45°
    Laser spot of uncoated Fe2+∶ZnSe crystal. (a) Normal incident; (b) 45° incident
    • Table 1. Parameters of Fe∶ZnSe crystal samples

      View table

      Table 1. Parameters of Fe∶ZnSe crystal samples

      Sample IDThickness /mm

      Cross section /

      (mm×mm)

      Coating

      status

      Doped uniformity
      13.008×9CoatedGood
      26.00
      33.5627×8UncoatedBad
    Tools

    Get Citation

    Copy Citation Text

    Hao Liu, Kenan Wu, Yuqi Jin. Long-Pulse Output Characteristics of Solid-State Fe2+∶ZnSe Laser at Low Temperature[J]. Laser & Optoelectronics Progress, 2024, 61(17): 1714008

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: Lasers and Laser Optics

    Received: Jan. 30, 2024

    Accepted: Apr. 28, 2024

    Published Online: Sep. 14, 2024

    The Author Email: Kenan Wu (wukn@dicp.ac.cn), Yuqi Jin (yqjin@dicp.ac.cn)

    DOI:10.3788/LOP240637

    CSTR:32186.14.LOP240637

    Topics