Bulletin of the Chinese Ceramic Society, Volume. 44, Issue 6, 2337(2025)

Effects of Different Lactates on Hydration Process of MgO

ZHOU Jing1,2, WANG Zhoufu1、*, LIU Hao1,2, MA Yan1,2, and WANG Xitang1
Author Affiliations
  • 1The State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China
  • 2The State Key Laboratory of Advanced Refractories, Wuhan University of Science and Technology, Wuhan 430081, China
  • show less
    References(13)

    [4] [4] CAI M F, LIANG Y H, YIN Y C, et al. Effect of citric acid on the hydration process of colloidal silica-bonded magnesia gunning materials[J]. Ceramics International, 2019, 45(12): 15514-15519.

    [5] [5] INOUE R, UCHIDATE M, KUSUKAWA S, et al. Control of hydration of free magnesia in steelmaking slag[J]. Journal of Sustainable Metallurgy, 2021, 7(3): 818-830.

    [7] [7] ZHANG W Z, CHEN B, MOU J N, et al. Improved hydration resistance of magnesia by EDTA and ammonium phosphate as additives[J]. Science and Engineering of Composite Materials, 2017, 24(1): 29-33.

    [8] [8] DOS SANTOS T, DOS SANTOS J, LUZ A P, et al. Kinetic control of MgO hydration in refractory castables by using carboxylic acids[J]. Journal of the European Ceramic Society, 2018, 38(4): 2152-2163.

    [9] [9] FINI D S, MIGUEL V C, PINTO V S, et al. Aluminum lactate role in improving hydration and drying behavior of MgO-bonded refractory castables[J]. Ceramics International, 2020, 46(10): 17093-17102.

    [10] [10] MIGUEL V C, FINI D S, PINTO V S, et al. Crack-free caustic magnesia-bonded refractory castables[J]. Ceramics International, 2021, 47(12): 17255-17261.

    [11] [11] PINTO V S, FINI D S, MIGUEL V C, et al. Fast drying of high-alumina MgO-bonded refractory castables[J]. Ceramics International, 2020, 46(8): 11137-11148.

    [12] [12] KOGA Y, SATO M, SEKIGUCHI K, et al. Effects of alumina cement grade and additives on alumina-magnesia castables containing aluminum lactate[J]. Taikabutsu Overseas, 1998, 18: 43-47.

    [15] [15] BAI L M, WANG M J, LIANG X Z, et al. Research on growth mechanism of magnesium hydroxide crystal thin films based on hydrothermal system[J]. Journal of Crystal Growth, 2024, 643: 127810.

    [16] [16] LIN S N, ZHANG T A, YANG H. Preparation and mechanism analysis of nano-Mg(OH)2 by electroconversion of MgCl2[J]. Fullerenes Nanotubes and Carbon Nanostructures, 2023, 31(7): 667-674.

    [17] [17] PANG H C, NING G L, GONG W T, et al. Directed tuning of nanostructure from 1D to 3D by doping diverse valent cations[J]. RSC Advances, 2011, 1(2): 184.

    [18] [18] CHEN L, JIANG L H, CHU H Q, et al. Effect of retarder on hydration properties of light-burned magnesia[J]. Construction and Building Materials, 2020, 263: 119762.

    [19] [19] AMARAL L F, OLIVEIRA I R, BONADIA P, et al. Chelants to inhibit magnesia (MgO) hydration[J]. Ceramics International, 2011, 37(5): 1537-1542.

    Tools

    Get Citation

    Copy Citation Text

    ZHOU Jing, WANG Zhoufu, LIU Hao, MA Yan, WANG Xitang. Effects of Different Lactates on Hydration Process of MgO[J]. Bulletin of the Chinese Ceramic Society, 2025, 44(6): 2337

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category:

    Received: Nov. 1, 2024

    Accepted: Jul. 30, 2025

    Published Online: Jul. 30, 2025

    The Author Email: WANG Zhoufu (whwangzf@126.com)

    DOI:10.16552/j.cnki.issn1001-1625.2024.1312

    Topics