Chinese Journal of Lasers, Volume. 47, Issue 11, 1102002(2020)

Microstructures and Mechanical Properties of 30CrMnSiA and 30CrMnSiNi2A High-Strength Steels After Laser-Cladding Repair

Pang Xiaotong1, Gong Qunfu2, Wang Zhijie2, Li Zhuguo1, and Yao Chengwu1、*
Author Affiliations
  • 1Shanghai Key Laboratory of Materials Laser Processing and Modification, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
  • 2PLA 4724 Plant, Shanghai 200436, China
  • show less
    References(29)

    [1] Yang S D. Formation causes and suppression of cracking in laser-MAG hybrid welding of 30CrMnSiA steel[D]. Harbin: Harbin Institute of Technology, 1-9(2012).

    [4] Da Sun S, Fabijanic D, Barr C et al. In-situ quench and tempering for microstructure control and enhanced mechanical properties of laser cladded AISI 420 stainless steel powder on 300M steel substrates[J]. Surface and Coatings Technology, 333, 210-219(2018).

    [6] Liu J, Li J, Cheng X et al. Microstructures and tensile properties of laser cladded AerMet100 steel coating on 300M steel[J]. Journal of Materials Science & Technology, 34, 643-652(2018).

    [7] Rahman Rashid R A, Nazari K A, Barr C et al. Effect of laser reheat post-treatment on the microstructural characteristics of laser-cladded ultra-high strength steel[J]. Surface and Coatings Technology, 372, 93-102(2019).

    [8] Rahman Rashid R A, Barr C J, Palanisamy S et al. Effect of clad orientation on the mechanical properties of laser-clad repaired ultra-high strength 300M steel[J]. Surface and Coatings Technology, 380, 125090(2019).

    [9] Barr C, Da Sun S, Easton M et al. Influence of delay strategies and residual heat on in situ tempering in the laser metal deposition of 300M high strength steel[J]. Surface and Coatings Technology, 383, 125279(2020).

    [11] Lourenço J M, Sun S D, Sharp K et al. Fatigue and fracture behavior of laser clad repair of AerMet ® 100 ultra-high strength steel[J]. International Journal of Fatigue, 85, 18-30(2016).

    [12] Walker K F, Lourenço J M, Sun S et al. Quantitative fractography and modelling of fatigue crack propagation in high strength AerMet® 100 steel repaired with a laser cladding process[J]. International Journal of Fatigue, 94, 288-301(2017).

    [13] Barr C, Da Sun S, Easton M et al. Influence of macrosegregation on solidification cracking in laser clad ultra-high strength steels[J]. Surface and Coatings Technology, 340, 126-136(2018).

    [14] Sun S D, Liu Q C, Brandt M et al. Effect of laser clad repair on the fatigue behaviour of ultra-high strength AISI 4340 steel[J]. Materials Science and Engineering A, 606, 46-57(2014).

    [15] Chew Y. Pang J H L, Bi G J, et al. Effects of laser cladding on fatigue performance of AISI 4340 steel in the as-clad and machine treated conditions[J]. Journal of Materials Processing Technology, 243, 246-257(2017).

    [16] Sun G F, Yao S, Wang Z D et al. Microstructure and mechanical properties of HSLA-100 steel repaired by laser metal deposition[J]. Surface and Coatings Technology, 351, 198-211(2018).

    [17] Li W Q. Laser cladding intensification on 30CrMnSi surface[J]. Special Casting & Nonferrous Alloys, 39, 1058-1061(2019).

    [18] Zhang Z Q, Qin R Y, Sun T et al. Microstructure and properties of laser cladding joints of 30CrMnSiA steel[J]. Welding Technology, 47, 9-14(2018).

    [20] Zhang Z Q, Cheng Z H, Cao Q et al. Repairing of 30CrMnSiNi2A high strength steel by laser cladding[J]. Equipment Environmental Engineering, 13, 62-67(2016).

    [21] Zhu H M, Hu J P, Li B C et al. Research progress of laser cladding stainless steel coating on Fe-based substrate[J]. Surface Technology, 49, 74-84(2020).

    [22] Lei Z L, Li B W, Ni L C et al. Mechanism of the crack formation and suppression in laser-MAG hybrid welded 30CrMnSiA joints[J]. Journal of Materials Processing Technology, 239, 187-194(2017).

    [24] Chipman J. Thermodynamics and phase diagram of the Fe-C system[J]. Metallurgical and Materials Transactions B, 3, 55-64(1972).

    [25] Su T J, Wang F C, Li S K et al. Calculation of thermal conductivity for alloy steels[J]. Transactions of Beijing Institute of Technology, 25, 91-94(2005).

    [27] Sattar A, Abbas M, Hasham H J et al. Experimental and analytical investigation of steel bolts failed after isothermal heat treatment[J]. Journal of Failure Analysis and Prevention, 15, 327-333(2015).

    [28] Liu B X, Chen C X, Yin F X et al[M]. Microstructure analysis and weldability investigation of stainless steel clad plate, 425-433(2017).

    Tools

    Get Citation

    Copy Citation Text

    Pang Xiaotong, Gong Qunfu, Wang Zhijie, Li Zhuguo, Yao Chengwu. Microstructures and Mechanical Properties of 30CrMnSiA and 30CrMnSiNi2A High-Strength Steels After Laser-Cladding Repair[J]. Chinese Journal of Lasers, 2020, 47(11): 1102002

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: laser manufacturing

    Received: Apr. 20, 2020

    Accepted: --

    Published Online: Nov. 11, 2020

    The Author Email: Chengwu Yao (yaochwu@sjtu.edu.cn)

    DOI:10.3788/CJL202047.1102002

    Topics