Chinese Journal of Lasers, Volume. 47, Issue 12, 1214001(2020)

Terahertz Dielectric Spectra for Thermal Oxygen Aging of Natural Rubber

Zhang Xiansheng1, Chang Tianying1、*, Cui Hongliang2, Liu Lingyu1, and Li Yizhang1
Author Affiliations
  • 1Institute of Automation, Shandong Academy of Sciences, Jinan, Shandong 250014, China
  • 2Chongqing Institute of Green Intelligence, Chinese Academy of Sciences, Chongqing 400714, China
  • show less
    References(31)

    [1] Men X, Wang F, Chen G Q et al. Biosynthesis of natural rubber: current state and perspectives[J]. International Journal of Molecular Sciences, 20, 50(2018).

    [5] Li G Y, Koenig J L. A review of rubber oxidation[J]. Rubber Chemistry and Technology, 78, 355-390(2005).

    [6] Nie J D, Huang X H, Xu C H et al. Antioxidant effects on curing/processing and thermo-oxidative aging of filled nitrile rubber[J]. Materials Chemistry and Physics, 253, 123403(2020).

    [10] Kuwahara H, Sudo S, Iijima M et al. Dielectric properties of thermally degraded chloroprene rubber[J]. Polymer Degradation and Stability, 95, 2461-2466(2010).

    [12] Wietzke S, Jansen C, Reuter M et al. Terahertz spectroscopy on polymers: a review of morphological studies[J]. Journal of Molecular Structure, 1006, 41-51(2011).

    [15] Chang T Y, Zhang X S, Cui H L. Evolution of terahertz dielectric permittivity of rubber during thermo-oxidative aging[J]. Microwave and Optical Technology Letters, 60, 127-134(2018).

    [17] Withayachumnankul W, Naftaly M. Fundamentals of measurement in terahertz time-domain spectroscopy[J]. Journal of Infrared, Millimeter, and Terahertz Waves, 35, 610-637(2014).

    [20] Komethi M, Othman N, Ismail H et al. Comparative study on natural antioxidant as an aging retardant for natural rubber vulcanizates[J]. Journal of Applied Polymer Science, 124, 1490-1500(2012).

    [21] Zheng W, Liu L, Zhao X Y et al. Effects of lanthanum complex on the thermo-oxidative aging of natural rubber[J]. Polymer Degradation and Stability, 120, 377-383(2015).

    [22] Committee D. Test method for rubber-deterioration by heat and oxygen: ASTM D572-04[S]. West Conshohocken, PA: ASTM International(2010).

    [23] Rajesh K R, Menon C S. Estimation of the refractive index and dielectric constants of magnesium phthalocyanine thin films from its optical studies[J]. Materials Letters, 53, 329-332(2002).

    [24] Cardarelli F. Materials handbook: a concise desktop reference[M]. 2nd ed. London: Springer-Verlag, 716(2008).

    [27] Stewart J E, Linnig F J. The far infrared spectrum of vulcanized natural rubber[J]. Journal of Research of the National Bureau of Standards Section A: Physics and Chemistry, 71A, 19(1967).

    [28] Grasland F, Chazeau L, Chenal J M et al. About thermo-oxidative ageing at moderate temperature of conventionally vulcanized natural rubber[J]. Polymer Degradation and Stability, 161, 74-84(2019).

    [29] Zhao C, Zhao C Z, Werner M et al. Dielectric relaxation of high-k oxides[J]. Nanoscale Research Letters, 8, 456(2013).

    [30] Oughstun K E, Cartwright N A. On the Lorentz-Lorenz formula and the Lorentz model of dielectric dispersion[J]. Optics Express, 11, 1541-1546(2003).

    Tools

    Get Citation

    Copy Citation Text

    Zhang Xiansheng, Chang Tianying, Cui Hongliang, Liu Lingyu, Li Yizhang. Terahertz Dielectric Spectra for Thermal Oxygen Aging of Natural Rubber[J]. Chinese Journal of Lasers, 2020, 47(12): 1214001

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: terahertz technology

    Received: Jun. 29, 2020

    Accepted: --

    Published Online: Nov. 30, 2020

    The Author Email: Tianying Chang (tchang@jlu.edu.cn)

    DOI:10.3788/CJL202047.1214001

    Topics