Chinese Journal of Lasers, Volume. 49, Issue 8, 0802019(2022)
Microstructure Evolution and Nanocrystal Formation of TC4 by Laser Shock Peening
[1] Wang J, Li M, Wang J X et al. Effects of laser shock processing on fatigue life of 304 stainless steel[J]. Chinese Journal of Lasers, 46, 0102003(2019).
[2] Liu Y P, Shi Z J, Zhao Y Z et al. Cut-off value of detail fatigue rated strength of TC4 titanium alloy with compound strengthening treatment by laser shock peening and shot peening[J]. Chinese Journal of Lasers, 47, 0502006(2020).
[3] Liu Y G, Li H M, Li M Q. Characterization of surface layer in TC17 alloy treated by air blast shot peening[J]. Materials & Design (1980-2015), 65, 120-126(2015).
[4] Wang Y L, Bian X F, Fu B et al. Surface integrity and fatigue behaviour of holes treated by finishing & burnishing and split sleeve cold expansion[J]. Surface Technology, 48, 336-345(2019).
[5] Qiao H C, Hu X L, Zhao J B et al. Influence parameters and development application of laser shock processing[J]. Surface Technology, 48, 1-9, 53(2019).
[6] Li Y H, He W F, Zhou L C. The strengthening mechanism of laser shock processing and its application on the aero-engine components[J]. Scientia Sinica Technologica, 45, 1-8(2015).
[7] Yang J D, Zhou W F, Yang T et al. Nanocrystallization of Ti-6Al-4V alloy by multiple laser shock processing[J]. Laser Technology, 41, 754-758(2017).
[8] Nie X F, He W F, Zang S L et al. Experimental study on improving high-cycle fatigue performance of TC11 titanium alloy by laser shock peening[J]. Chinese Journal of Lasers, 40, 0803006(2013).
[9] Liu H X, Hu Y, Wang X et al. Grain refinement progress of pure titanium during laser shock forming (LSF) and mechanical property characterizations with nanoindentation[J]. Materials Science and Engineering: A, 564, 13-21(2013).
[10] Che Z G, Yang J, Gong S L et al. Self-nanocrystallization of Ti-6Al-4V alloy surface induced by laser shock processing[J]. Rare Metal Materials and Engineering, 43, 1056-1060(2014).
[11] Nie X F, He W F, Zhou L C et al. Experiment investigation of laser shock peening on TC6 titanium alloy to improve high cycle fatigue performance[J]. Materials Science and Engineering: A, 594, 161-167(2014).
[12] Nie X F, He W F, Zang S L et al. Effect study and application to improve high cycle fatigue resistance of TC11 titanium alloy by laser shock peening with multiple impacts[J]. Surface and Coatings Technology, 253, 68-75(2014).
[13] Altenberger I, Nalla R K, Sano Y et al. On the effect of deep-rolling and laser-peening on the stress-controlled low- and high-cycle fatigue behavior of Ti-6Al-4V at elevated temperatures up to 550 ℃[J]. International Journal of Fatigue, 44, 292-302(2012).
[14] Yang Y, Zhou K, Zhang H et al. Thermal stability of microstructures induced by laser shock peening in TC17 titanium alloy[J]. Journal of Alloys and Compounds, 767, 253-258(2018).
[15] Chen K M, Zheng C C, Yuan Z Z et al. Deformation microstructures of austenitic stainless steel 2Cr13Mn9Ni4 under ultrafast strain rate by laser shock processing[J]. Materials Science and Engineering: A, 587, 244-249(2013).
[16] Trdan U, Skarba M, Grum J. Laser shock peening effect on the dislocation transitions and grain refinement of Al-Mg-Si alloy[J]. Materials Characterization, 97, 57-68(2014).
[17] Jiang C Y, Wang C Y, Luo K Y et al. Effects of laser shock layer number and Cl-concentration on anticorrosion behaviors of AM50 Mg alloys[J]. Chinese Journal of Lasers, 45, 0902004(2018).
[18] Chen X Z, Wang J J, Fang Y Y et al. Investigation of microstructures and residual stresses in laser peened Incoloy 800H weldments[J]. Optics & Laser Technology, 57, 159-164(2014).
[19] Wang X, Xia W G, Wu X Q et al. Microstructure and mechanical properties of an austenite NiTi shape memory alloy treated with laser induced shock[J]. Materials Science and Engineering: A, 578, 1-5(2013).
[20] Zhou Z, Gill A S, Telang A et al. Experimental and finite element simulation study of thermal relaxation of residual stresses in laser shock peened IN718 SPF superalloy[J]. Experimental Mechanics, 54, 1597-1611(2014).
[21] Hatamleh O, Rivero I V, Swain S E. An investigation of the residual stress characterization and relaxation in peened friction stir welded aluminum-lithium alloy joints[J]. Materials & Design, 30, 3367-3373(2009).
[22] Li Y H[M]. Theory and technology of laser shock peening, 209-228(2013).
[23] Lainé S J, Knowles K M, Doorbar P J et al. Microstructural characterisation of metallic shot peened and laser shock peened Ti-6Al-4V[J]. Acta Materialia, 123, 350-361(2017).
[24] Pan X L, Xu D W, Tian Z et al. Effect of dynamic recrystallization on texture orientation and grain refinement of Ti6Al4V titanium alloy subjected to laser shock peening[J]. Journal of Alloys and Compounds, 850, 156672(2021).
Get Citation
Copy Citation Text
Bohan Wang, Li Cheng, Dongchun Li. Microstructure Evolution and Nanocrystal Formation of TC4 by Laser Shock Peening[J]. Chinese Journal of Lasers, 2022, 49(8): 0802019
Category: laser manufacturing
Received: Aug. 13, 2021
Accepted: Nov. 3, 2021
Published Online: Mar. 23, 2022
The Author Email: Bohan Wang (dream0729ing@foxmail.com)