Chinese Journal of Lasers, Volume. 47, Issue 11, 1102007(2020)

Effect of Nanosecond Laser-Induced Micro-Nanostructures on Biocompatibility of Zr-Based Bulk Metallic Glasses

Jiao Yang1、*, He Weifeng1, Shangguan Long2, Zhou Liucheng1, Luo Sihai1, and Nie Xiangfan1
Author Affiliations
  • 1Science and Technology on Plasma Dynamics Laboratory, Aeronautics Engineering College, Air Force Engineering University, Xi''an, Shaanxi 710043, China
  • 2Orthopedics Department, Jingyang County Hospital, Shaanxi Province, Xianyang, Shaanxi 713700, China
  • show less
    Figures & Tables(9)
    Nanosecond laser system and schematic of surface textures (dimple and groove)
    Surface 3D morphologies of different Zr-based bulk metallic glasses. (a) Original sample; (b) dimple-textured sample; (c) groove-textured sample
    Scanning electron microscope images of different Zr-based bulk metallic glasses surfaces. (a)(b) Original sample; (c)(d) dimple-textured sample; (e)(f) groove-textured sample
    Cell viability of MG-63 cells cultured on different Zr-based bulk metallic glasses surfaces for 24 h (AC: original sample, GT: groove-textured sample, DT: dimple-textured)
    Distribution and morphology of MG-63 cells on different Zr-based bulk metallic glasses samples surfaces. (a) Original sample; (b) groove-textured sample; (c) dimple-textured sample
    • Table 1. Main chemical composition of Vitreloy 105 Zr-based bulk metallic glasses

      View table

      Table 1. Main chemical composition of Vitreloy 105 Zr-based bulk metallic glasses

      ElementZrCuNiAlTi
      Volume fraction /%52.817.614.89.94.9
    • Table 2. Laser parameters for the fabrication of two surface micro-nano structures

      View table

      Table 2. Laser parameters for the fabrication of two surface micro-nano structures

      ParameterValue
      Wavelength /nm1064
      Spot diameter /μm32
      Pulse duration /ns220
      Frequency /kHz20
      Laser fluence /(J·cm-2)30
      Track distance /μm90
      Scanning speed /(mm·s-1)0 (dimples)200 (grooves)
    • Table 3. Dimensions of surface textures and surface roughness of different samples

      View table

      Table 3. Dimensions of surface textures and surface roughness of different samples

      SampleSurfaceroughness /μmDepth /μmDiameter orwidth /μm
      Dimple-textured0.212.4432.23
      Groove-textured3.5410.228.6
      Original0.065--
    • Table 4. Chemical composition of different Zr-based bulk metallic glasses surfaces

      View table

      Table 4. Chemical composition of different Zr-based bulk metallic glasses surfaces

      SampleAtomic fraction /%
      COZrCuNiAlTi
      Original58.8928.584.770.760.445.690.87
      Dimple-textured72.8718.231.330.830.365.690.70
      Groove-textured75.4617.121.080.730.384.580.66
    Tools

    Get Citation

    Copy Citation Text

    Jiao Yang, He Weifeng, Shangguan Long, Zhou Liucheng, Luo Sihai, Nie Xiangfan. Effect of Nanosecond Laser-Induced Micro-Nanostructures on Biocompatibility of Zr-Based Bulk Metallic Glasses[J]. Chinese Journal of Lasers, 2020, 47(11): 1102007

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: laser manufacturing

    Received: May. 18, 2020

    Accepted: --

    Published Online: Nov. 2, 2020

    The Author Email: Yang Jiao (young_joeafeu@163.com)

    DOI:10.3788/CJL202047.1102007

    Topics