Acta Optica Sinica, Volume. 43, Issue 7, 0716002(2023)
Process of Sc/Zr-Modified Al-Mg Alloy Prepared by Additive/Equivalent Composite Manufacturing
[1] Gu D D, Zhang H M, Chen H Y et al. Laser additive manufacturing of high-performance metallic aerospace components[J]. Chinese Journal of Lasers, 47, 0500002(2020).
[2] Qin Y L, Sun B H, Zhang H et al. Development of selective laser melted aluminum alloys and aluminum matrix composites in aerospace field[J]. Chinese Journal of Lasers, 48, 1402002(2021).
[3] He P, Bai X W, Zhou X M et al. Microstructure and properties of 6061 aluminum alloy by MIG wire and arc additive manufacturing[J]. Transactions of the China Welding Institution, 43, 50-54, 60, 116(2022).
[4] Debroy T, Wei H L, Zuback J et al. Additive manufacturing of metallic components-process, structure and properties[J]. Progress in Materials Science, 92, 112-224(2018).
[5] Brice C, Shenoy R, Kral M. Precipitation behavior of aluminum alloy 2139 fabricated using additive manufacturing[J]. Materials Science and Engineering A, 648, 9-14(2015).
[6] Atzeni E, Salmi A. Economics of additive manufacturing for end-usable metal parts[J]. The International Journal of Advanced Manufacturing Technology, 62, 1147-1155(2012).
[7] Svetlizky D, Das M, Zheng B et al. Directed energy deposition (DED) additive manufacturing: physical characteristics, defects, challenges and applications[J]. Materials Today, 49, 271-295(2021).
[8] Thompson S M, Bian L K, Shamsaei N et al. An overview of Direct Laser Deposition for additive manufacturing; Part I: transport phenomena, modeling and diagnostics[J]. Additive Manufacturing, 8, 36-62(2015).
[9] Thompson S M, Bian L K, Shamsaei N et al. An overview of Direct Laser Deposition for additive manufacturing; Part Ⅱ: mechanical behavior, process parameter optimization and control[J]. Additive Manufacturing, 8, 12-35(2015).
[10] Kang Y, Zhao Y Q, Li Y et al. Effect of driving force on molten pool behavior of 2219 aluminum alloy DLBSW process[J]. Transactions of the China Welding Institution, 43, 82-87, 118(2022).
[11] Sun C S, Zhang Z D, Liu L M. Effect of laser power on microstructure and properties of 5356 aluminum alloy by laser induced MIG arc additive manufacturing[J]. Transactions of the China Welding Institution, 39, 13-18, 129(2018).
[12] Li R D, Wang M B, Li Z M et al. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms[J]. Acta Materialia, 193, 83-98(2020).
[13] Lei Z L, Bi J, Chen Y B et al. Effect of energy density on formability, microstructure and micro-hardness of selective laser melted Sc- and Zr- modified 7075 aluminum alloy[J]. Powder Technology, 356, 594-606(2019).
[14] Gu J L, Ding J, Williams S W et al. The strengthening effect of inter-layer cold working and post-deposition heat treatment on the additively manufactured Al-6.3Cu alloy[J]. Materials Science and Engineering A, 651, 18-26(2016).
[15] Bai J Y, Fan C L, Lin S B et al. Mechanical properties and fracture behaviors of GTA-additive manufactured 2219-Al after an especial heat treatment[J]. Journal of Materials Engineering and Performance, 26, 1808-1816(2017).
[16] Zhong H, Qi B J, Cong B Q et al. Microstructure and mechanical properties of wire+arc additively manufactured 2050 Al-Li alloy wall deposits[J]. Chinese Journal of Mechanical Engineering, 32, 184-190(2019).
[17] McPherson J W, Dunn C F. A model for stress-induced metal notching and voiding in very large-scale-integrated Al-Si (1%) metallization[J]. Journal of Vacuum Science & Technology B, 5, 1321-1325(1987).
[18] Toda H, Qu P C, Ito S et al. Formation behaviour of blister in cast aluminium alloy[J]. International Journal of Cast Metals Research, 27, 369-377(2014).
[19] Zhou Y H, Lin X, Kang N et al. Influence of travel speed on microstructure and mechanical properties of wire+arc additively manufactured 2219 aluminum alloy[J]. Journal of Materials Science & Technology, 37, 143-153(2020).
[20] Gu J L, Gao M J, Yang S L et al. Microstructure, defects, and mechanical properties of wire+arc additively manufactured AlCu4.3-Mg1.5 alloy[J]. Materials & Design, 186, 108357(2020).
[21] Zhang Y B, Xu J, Zhai T et al. Distributions of pore size and fatigue weak link strength in an A713 sand cast aluminum alloy[J]. Materials Science and Engineering: A, 527, 3639-3644(2010).
[22] Boeira A P, Ferreira I L, Garcia A. Alloy composition and metal/mold heat transfer efficiency affecting inverse segregation and porosity of as-cast Al-Cu alloys[J]. Materials & Design, 30, 2090-2098(2009).
Get Citation
Copy Citation Text
Yuhui Zhao, Chen He, Jibin Zhao, Jian Zou, Zhiguo Wang, Zhenfeng He. Process of Sc/Zr-Modified Al-Mg Alloy Prepared by Additive/Equivalent Composite Manufacturing[J]. Acta Optica Sinica, 2023, 43(7): 0716002
Category: Materials
Received: Sep. 2, 2022
Accepted: Nov. 25, 2022
Published Online: Apr. 6, 2023
The Author Email: He Chen (hechen@sia.cn)