Journal of Inorganic Materials, Volume. 40, Issue 2, 177(2025)

Preparation and Performance of Sintered SiC Fiber-bonded Ceramics

Wei LI, Zhiming XU, Yanzi GOU, Senhu YIN, Yiping YU, and Song WANG*
Author Affiliations
  • Science and Technology on Advanced Ceramic Fiber and Composites Laboratory, College of Aerospace Science and Engineering, National University of Defense Technology, Changsha 410073, China
  • show less
    References(22)

    [1] YIN F, RAO A G. Performance analysis of an aero engine with inter-stage turbine burner[J]. The Aeronautical Journal, 1605(2017).

    [2] SRINIVAS G, RAGHUNANDANA K, SATISH SHENOY B. Recent developments in turbomachinery component materials and manufacturing challenges for aero engine applications[conf-proc]. IOP Conference Series: Materials Science and Engineering, 012012(2018).

    [3] LIN Z M. The current development and future trends of fighter engines[J]. Aeroengine, 1(2006).

    [4] BERGS T, GRÜNEBAUM T, FRICKE K et al. Life cycle assessment for milling of Ti-and Ni-based alloy aero engine components[J]. Procedia CIRP, 625(2021).

    [5] WANG X G, LIU J L, JIN T et al. Tensile behaviors and deformation mechanisms of a nickel-base single crystal superalloy at different temperatures[J]. Materials Science and Engineering: A, 154(2014).

    [7] FAN X, YIN X. Progress in research and development on matrix modification of continuous fiber-reinforced silicon carbide matrix composites[J]. Advanced Composites and Hybrid Materials, 685(2018).

    [9] KARADIMAS G, SALONITIS K. Ceramic matrix composites for aero engine applications--a review[J]. Applied Sciences, 3017(2023).

    [10] KATOH Y, SNEAD L L, HENAGER J C H et al. Current status and recent research achievements in SiC/SiC composites[J]. Journal of Nuclear Materials, 387(2014).

    [11] DICARLO J A, YUN H M, MORSCHER G N et al[M]. SiC/SiC composites for 1200 ℃ and above//BANSAL N P. Handbook of ceramic composites, 77-98(2005).

    [12] LUTHRA K L, CORMAN G S. Melt infiltrated (MI) SiC/SiC composites for gas turbine applications//KRENKEL W, NASLAIN R, SCHNEIDER H. High temperature ceramic matrix composites[J]. Ohio: Wiley-American Ceramic Society, 744-753(2001).

    [14] ISHIKAWA T, KAJII S, MATSUNAGA K et al. A tough, thermally conductive silicon carbide composite with high strength up to 1600 ℃ in air[J]. Science, 1295(1998).

    [15] HO C Y, TSAI S C, LIN H T et al. Microstructural investigation of Si-ion-irradiated single crystal 3C-SiC and SA-Tyrannohex SiC fiber-bonded composite at high temperatures[J]. Journal of Nuclear Materials, 1(2013).

    [16] XU Z M, YU Y P, WANG S et al. Research progress of SiC fiber-bonded ceramics[J]. Journal of Material Engineering, 23(2023).

    [17] VERA M C, MARTÍNEZ-FERNÁNDEZ J, SINGH M et al. Strength and thermal shock resistance of Si-Al-C-O and Si-Ti-C-O fiber-bonded ceramics[J]. International Journal of Applied Ceramic Technology, 1126(2022).

    [18] GOU Y, WANG H, JIAN K. Formation of carbon-rich layer on the surface of SiC fiber by sintering under vacuum for superior mechanical and thermal properties[J]. Journal of the European Ceramic Society, 907(2017).

    [19] ZHANG Y, CHEN J, YAN D et al. Conversion of silicon carbide fibers to continuous graphene fibers by vacuum annealing[J]. Carbon, 435(2021).

    [21] YAMAMOTO H, BABA Y, SASAKI T A. Electronic structures of N2+ and O2+ ion-implanted Si (100)[J]. Surface and Interface Analysis, 381(1995).

    [22] KAJII S, MATSUNAGA K, SATO M et al. Mechanical behavior of SiC-Polycrystalline fiber-bonded-cermics[conf-proc]. 28th International Conference on Advanced Ceramics and Composites B:Ceramic Engineering and Science Proceedings, Hoboken, 43-48(2004).

    [23] CORMAN G S, LUTHRA K L[M]. Silicon melt infiltrated ceramic composites (HiPerComp™)//BANSAL N P. Handbook of ceramic composites, 99-115(2005).

    [24] ZHANG J, ZHANG Y, WANG Y et al. Long-term oxidation performance of SiCf/SiC composites at 1200 ℃ in air atmosphere manufactured by PIP and hybrid CVI/PIP techniques[J]. Ceramics International, 10259(2024).

    Tools

    Get Citation

    Copy Citation Text

    Wei LI, Zhiming XU, Yanzi GOU, Senhu YIN, Yiping YU, Song WANG. Preparation and Performance of Sintered SiC Fiber-bonded Ceramics[J]. Journal of Inorganic Materials, 2025, 40(2): 177

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category:

    Received: Jun. 17, 2024

    Accepted: --

    Published Online: Apr. 24, 2025

    The Author Email: Song WANG (wangs_0731@163.com)

    DOI:10.15541/jim20240292

    Topics