Journal of Inorganic Materials, Volume. 35, Issue 2, 211(2020)

Critical Size on Spontaneous Breakage of Tempered Glass Initiated by NiS Particle

Xiao-Gen LIU1...2, Yi-Wang BAO1,2, De-Tian WAN1,2 and Yu-Kang SUN2 |Show fewer author(s)
Author Affiliations
  • 1State Key Laboratory of Green Building Materials, China Building Materials Academy, Beijing 100024, China
  • 2China Building Material Test & Certification Group Co., Ltd, Beijing 100024, China
  • show less
    References(13)

    [1] W BAO Y, Q LIU Z. Mechanism and criterion of spontaneous breakage of tempered glass. Journal of Inorganic Materials, 31, 401-406(2016).

    [2] V SWAIN M. A fracture mechanism description of the microcracking about NiS inclusions in glass. Journal of Non-Crystalline Solids, 38-39, 451-456(1980).

    [3] V SWAIN M. Nickel sulfide inclusions in glass: an example of microcracking induced by a volumetric expanding phase change. Journal of Materials Science, 16, 151-158(1981).

    [4] J LEON. A Review of the Nickel Sulphide Induced Fracture in Tempered Glass. Proceeding on Glass Processing Days, Finland, 108-110(2001).

    [5] T TÖLKE, A BARZI, D STACHEL. Behaviour and phase transformations of nickel sulphide inclusions in glass melts. Journal of Physics and Chemistry of Solids, 68, 830-834(2007).

    [6] B JOHN C. A study of nickel sulphide stones in tempered glass. Ultramicroscopy, 52, 297-305(1993).

    [7] Y OUSSAMA, D PATRICIA, B YVES et al. Phase transformations in nickel sulphide: microstructures and mechanisms. Acta Materialia, 58, 3367-3380(2010).

    [8] W BISHOPA D, S THOMASA P, S RAYA A. Micro Raman characterization of nickel sulfide inclusions in toughened glass. Materials Research Bulletin, 35, 1123-1128(2010).

    [9] T WAN D, W BAO Y, X G J LIU et al. Spontaneous breakage source spontaneous breakage mechanism analysis and online testing technology on tempered glass used in door and window and curtain wall. China Building Materials Science & Technology, 2010, 178-184.

    [10] X LI, P FANG Z, I READING et al. In-situ Inspection of Inclusions in Toughened Glass Panels of High-rise Buildings. Third Intl. Conf. on Experimental Mechanics and Third Conf. of the Asian Committee on Experimental Mechanics, 134-139(2005).

    [13] W BAO Y, Z JIN. Size effects and a mean-strength criterion for ceramics. Fatigue & Fracture of Engineering Materials & Structures, 16, 829-835(1993).

    [14] M KOLLI, M HAMIDOUCHE, M BOUAOUDJA et al. HF etching effect on sandblasted soda-lime glass properties. Journal of the European Ceramic Society, 29, 2697-2704(2009).

    [15] S LU J, Z LIU W, L DU J et al. Effect of etching time on surface microstructure and properties of glass treated in a mixed acid solution. Journal of Nanchang Hangkong University: Natural Sciences, 27, 79-84(2013).

    Tools

    Get Citation

    Copy Citation Text

    Xiao-Gen LIU, Yi-Wang BAO, De-Tian WAN, Yu-Kang SUN. Critical Size on Spontaneous Breakage of Tempered Glass Initiated by NiS Particle[J]. Journal of Inorganic Materials, 2020, 35(2): 211

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: RESEARCH PAPER

    Received: Feb. 25, 2018

    Accepted: --

    Published Online: Jan. 27, 2021

    The Author Email:

    DOI:10.15541/jim20190082

    Topics