Moistureproof Film of Polymeric (CH3)2Si(OC2H5)2 on Phosphate Laser Glass

[in Chinese]*, [in Chinese], [in Chinese], and [in Chinese]
Author Affiliations
  • [in Chinese]
  • show less

    (CH3)2Si(OC2H5)2 as precursor, a sol of good stability is prepared by sol-gel method and organic synthesization. After the sol is coated it on phosphate laser glass by rotating way, moistureproof film is worked out, having a transmittance of 96.5% after heated. The film has a good morphology, roughness of mean square (RMS) of 1.659 nm and roughness of average (RA) of 1.321 nm. The damaged threshold of the moistureproof film is high to 10~14 J/cm2, tested by a laser of wavelength of 1053 nm and pulse width of 1 ns. In the period of 5 years on “Shenguang Ⅱ” high power laser equipment, it behaves good moistureproof performance , and tryouts on “Shenguang Ⅲ” model.

    Tools

    Get Citation

    Copy Citation Text

    [in Chinese], [in Chinese], [in Chinese], [in Chinese]. Moistureproof Film of Polymeric (CH3)2Si(OC2H5)2 on Phosphate Laser Glass[J]. Collection Of theses on high power laser and plasma physics, 2005, 3(1): 1577

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category:

    Received: Sep. 29, 2004

    Accepted: --

    Published Online: Jun. 1, 2007

    The Author Email: (liu_ruijun@163.com)

    DOI:

    Topics