Journal of Advanced Dielectrics, Volume. 11, Issue 6, 2150023(2021)
Pyroelectric properties of 91.5TiO3–8.5lead-free single crystal
Bo Zhang1, Renbing Sun1、*, Fang Wang1, Tangfu Feng1, Pengna Zhang1, and Haosu Luo2
Author Affiliations
1School of Materials and Chemical Engineering, Ningbo University of Technology, Ningbo, Zhejiang 315016, P. R. China2Key Laboratory of Inorganic Functional Materials and Devices, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Jiading, Shanghai 201800, P. R. Chinashow less
The dielectric and pyroelectric performances of 91.5TiO3–8.5TiO3 lead-free single crystal were investigated. The depolarization temperature of the crystal is about 153 C. Among the <001>, <110>, and <111> crystallographic orientations, the <111>-oriented crystal possesses the highest pyroelectric coefficient and the largest figures of merit, and the values of , , and are 5.63×10 C/m2 •K, 0.06 m2/C, and 21.5 Pa for the <111>-oriented crystal at room temperature. The and exhibit weak frequency dependence in the range of 100–300 Hz. With the increase of the temperature, the value of increases, while the value of decreases from 18 C to 103 C.The dielectric and pyroelectric performances of 91.5TiO3–8.5TiO3 lead-free single crystal were investigated. The depolarization temperature of the crystal is about 153 C. Among the <001>, <110>, and <111> crystallographic orientations, the <111>-oriented crystal possesses the highest pyroelectric coefficient and the largest figures of merit, and the values of , , and are 5.63×10 C/m2 •K, 0.06 m2/C, and 21.5 Pa for the <111>-oriented crystal at room temperature. The and exhibit weak frequency dependence in the range of 100–300 Hz. With the increase of the temperature, the value of increases, while the value of decreases from 18 C to 103 C.