Journal of the Chinese Ceramic Society, Volume. 52, Issue 8, 2495(2024)

Crystallization Behavior and Mechanical Properties of Zinc-Containing Yttrium Aluminosilicate Glasses

ZHENG Qingshuang1, CHEN Shenglin1, QIAO Ang1, WANG Mitang2, and TAO Haizheng1、*
Author Affiliations
  • 1[in Chinese]
  • 2[in Chinese]
  • show less
    References(17)

    [1] [1] HYATT M J, DAY D E. Glass properties in the yttria-alumina-silica system[J]. J Am Ceram Soc, 1987, 70(10): 283–287.

    [2] [2] ARITA I H, WILKINSON D S, PURDY G R. Crystallization of yttria-alumina-silica glasses[J]. J Am Ceram Soc, 1992, 75(12):3315–3320.

    [3] [3] ZHENG Q S, LIU Y C, LI M, et al. Crystallization behavior and IR structure of yttrium aluminosilicate glasses[J]. J Eur Ceram Soc, 2020,40(2): 463–471.

    [4] [4] WANG M T, ZHENG Q S, CHEN A Y, et al. Crystallization, thermal expansion and hardness of Y2O3-Al2O3-SiO2 glasses[J]. Ceram Int,2021, 47(17): 25059–25066.

    [5] [5] SUN L B, SHI X S, LIU X Y, et al. Joining of Cf/SiC composites and Si3N4 ceramic with Y2O3-Al2O3-SiO2 glass filler for high-temperature applications[J]. Ceram Int, 2021, 47(11): 15622–15630.

    [6] [6] GOZZELINO L, CASALEGNO V, GHIGO G, et al. He-irradiation effects on glass-ceramics for joining of SiC-based materials[J]. J Nucl Mater, 2016, 472: 28–34.

    [7] [7] MA Y J, YANG S B, MENG X Y, et al. Corrosion behavior and mechanism of the Y2O3-Al2O3-SiO2 system during long-term corrosion in water-oxygen environment at 1350℃[J]. Ceram Int, 2023, 49(17):28344–28353.

    [8] [8] FAN S W, LIU J L, MA X, et al. Microstructure and properties of SiCf/SiC joint brazed by Y-Al-Si-O glass[J]. Ceram Int, 2018, 44(7):8656–8663.

    [9] [9] WANG L, FAN S W, SUN H D, et al. Pressure-less joining of SiCf/SiC composites by Y2O3-Al2O3-SiO2 glass: Microstructure and properties[J]. Ceram Int, 2020, 46(17): 27046–27056.

    [10] [10] ZHU W W, JIANG H F, ZHANG H, et al. Effect of TiO2 and CaF2 on the crystallization behavior of Y2O3-Al2O3-SiO2 glass ceramics[J].Ceram Int, 2018, 44(6): 6653–6658.

    [11] [11] HERRMANN M, LIPPMANN W, HURTADO A. Y2O3-Al2O3-SiO2-based glass-ceramic fillers for the laser-supported joining of SiC[J]. J Eur Ceram Soc, 2014, 34(8): 1935–1948.

    [12] [12] ZHANG J M, CHEN X W, YANG J S, et al. Enhanced wet-oxidation resistance of Y2O3 modified SiC ceramics by the formation of Y2Si2O7 protective layer[J]. J Eur Ceram Soc, 2023, 43(11): 4616–4626.

    [13] [13] ESHELBY J D. The determination of the elastic field of an ellipsoidal inclusion, and related problems[J]. Proc R Soc Lond A, 1957,241(1226): 376–396.

    [14] [14] SERBENA F C, ZANOTTO E D. Internal residual stresses in glassceramics:A review[J]. J Non Cryst Solids, 2012, 358(6/7): 975–984.

    [16] [16] GUI H, LI C, LIN C W, et al. Glass forming, crystallization, and physical properties of MgO-Al2O3-SiO2-B2O3 glass-ceramics modified by ZnO replacing MgO[J]. J Eur Ceram Soc, 2019, 39(4): 1397–1410.

    [17] [17] American Society for Testing and Materials. ASTM C142—18 Standard Test Methods for Determination of Fracture Toughness of Advanced Ceramics at Ambient Temperature[S]. America: ASTM International, 2018.

    [18] [18] ALIZADEH T, SOLEIMANI F. Preparation of nano-glass ceramic in ZAS system without added nucleating agents[J]. J Non Cryst Solids,2019, 520: 119465.

    Tools

    Get Citation

    Copy Citation Text

    ZHENG Qingshuang, CHEN Shenglin, QIAO Ang, WANG Mitang, TAO Haizheng. Crystallization Behavior and Mechanical Properties of Zinc-Containing Yttrium Aluminosilicate Glasses[J]. Journal of the Chinese Ceramic Society, 2024, 52(8): 2495

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category:

    Received: Nov. 22, 2023

    Accepted: --

    Published Online: Dec. 4, 2024

    The Author Email: Haizheng TAO (thz@whut.edu.cn)

    DOI:10.14062/j.issn.0454-5648.20230897

    Topics