Infrared and Laser Engineering, Volume. 45, Issue 5, 521001(2016)

Preparation of oxide films in TM laser cavity mirrors with high damage threshold

Zhao Yang1,2, He Yu1,2, Jiao Hongfei1,2, Zhang Jinlong1,2, Cheng Xinbin1,2, Liu Huasong1,3, Li Gangzheng4, and Wu Xiaoming5
Author Affiliations
  • 1[in Chinese]
  • 2[in Chinese]
  • 3[in Chinese]
  • 4[in Chinese]
  • 5[in Chinese]
  • show less
    References(17)

    [1] [1] Singh U N, AByrd J, Wi11iams-Byrda N P, et al. Diode pumped 2-μm solid state lidar transmitter for wind measurements[C]//SPIE, 1997, 3104: 173-178.

    [2] [2] Koch G J, Dharamsi A N, Fitzgerald C M, et al. Frequency stabilization of Ho:Tm:YLF laser to absorption lines of carbon dioxide[J]. Applied Optics, 2000, 39(21): 3664-3669.

    [3] [3] Liu Peipei, Bai Yang, Ren Zhaoyu, et al. Research and progress of 2 μm fiber lasers[J]. Infrared and Laser Engineering, 2009, 38(1): 45-49. (in Chinese)

    [4] [4] Zhang Xiurong, Fan Ruiying, Wu Guangzhao, et al. The damage of dielectric mirrors from 2.94 μm laser beams in YAG: Er3+ crystal [J]. Laser Technology, 1991, 15(6): 382-384. (in Chinese)

    [6] [6] Lewis K L, Pitt A M, Corbett M, et al. Progress in optical coatings for the mid-infrared[C]//SPIE, 1997, 2966: 166-177.

    [7] [7] Milward J R, Lewis K, Pitt A M, et al. Laser damage issues for mid-IR optical parametric oscillator mirrors[C]//SPIE, 1994, 2114: 220-230.

    [9] [9] Wang Ying. Research on the fabrication of mid-infrared dielectric coatings for laser system[D]. Hangzhou: Zhejiang University, 2009: 9-10. (in Chinese)

    [10] [10] Li Dan, Zhu Ziqiang, Fu Xiongying, et al. Relations between the laser induced damage to optical thin film and the material band-gap[J]. Opto-Electronic Engineering, 1999, 26(4): 58-62. (in Chinese)

    [11] [11] Mero M, Liu Jianhua, Zeller J, et al. Femtosecond pulse damage behavior of oxide dielectric thin films[C]//SPIE, 2004, 5273: 8-16.

    [14] [14] Liu Huasong, Wang Lishuan, Jiang Chenghui, et al. Dispersive properties of optical constants of SiO2 films in the visible and infrared regions[J]. Acta Optica Sinica, 2013, 33(10): 308-313. (in Chinese)

    [15] [15] Liu Huasong, Ji Yiqin, Zhang Feng, et al. Dispersive properties of optical constants of some metallic oxide thin films in the mid-infrared regions[J]. Acta Optica Sinica, 2014, 34(8): 0831003. (in Chinese)

    [16] [16] Rahe M, Ristau D, Schmidt H. The effect of hydrogen concentration in conventional and IAD coatings on the absorption and laser induced damage at 10.6 μm[C]//SPIE, 1992, 1848: 335-348.

    [17] [17] Ai Wanjun, Xiong Shengming. Characterization of hafnia thin films made with different deposition technologies[C]//SPIE, 2011, 8190: 81900J.

    [18] [18] Gross T, Dreschau F, Ristau D, et al. Characterization of laser components for high-power Ho:YAG lasers [C]//SPIE, 1998, 3244: 111-117.

    Tools

    Get Citation

    Copy Citation Text

    Zhao Yang, He Yu, Jiao Hongfei, Zhang Jinlong, Cheng Xinbin, Liu Huasong, Li Gangzheng, Wu Xiaoming. Preparation of oxide films in TM laser cavity mirrors with high damage threshold[J]. Infrared and Laser Engineering, 2016, 45(5): 521001

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: 先进光学材料

    Received: Sep. 17, 2015

    Accepted: Oct. 21, 2015

    Published Online: Jun. 12, 2016

    The Author Email:

    DOI:10.3788/irla201645.0521001

    Topics