Development of the aluminum substrate reflective film in the off-axis three-mirror optical system

Pengquan Zhang1, Jiaqi Chen1, and Yijun Shi2
Author Affiliations
  • 1School of Electronics and Information, Hangzhou Dianzi University, Hangzhou 310018, China
  • 2Tianjin Bright Star Technology Co., Ltd, Tianjin 300192, China
  • show less
    Figures & Tables(8)
    Off-axis three-mirror optical system
    MTF curve
    Theoretical design curve of S- and P-light reflectivity at the incidence of 38.5°
    Theoretical design curve S- and P-light reflection phase at the incidence of 38.5°
    Experimental results of coated mirrors
    • Table 1. Main technical specifications of the off-axis three-mirror optical system

      View table
      View in Article

      Table 1. Main technical specifications of the off-axis three-mirror optical system

      ParametersValue
      Wavelength/nm1550
      Field of view/mrad15
      Magnification
      Entrance pupil diameter/mm125
      Isolation>80 dB
    • Table 2. Technical specifications of mirrors in the off-axis three-mirror optical system

      View table
      View in Article

      Table 2. Technical specifications of mirrors in the off-axis three-mirror optical system

      ParametersParameter values
      Incident angle/(°)38.5
      P- and S-light phase delay<1°@1550 nm
      Film polarization>99.5%@(1550±5) nm
    • Table 3. Test methods and results of film environment

      View table
      View in Article

      Table 3. Test methods and results of film environment

      ItemsResultsMethods
      Adhesion testNo stripping after pulling the 2 cm-zwide tape up from the film Stick a piece of 2 cm-wide adhesive tape (peel strength≥2.74 N/cm) firmly onto the surface of the film layer of the test piece, and pull up quickly.
      Damp heat test ① (50±2) ℃, 95-100%, 24 h; ② No peeling, stripping, cracking or bubbling on the film layer after the test. Keep the test piece in an environment 95%-100% in humidity and (50±2) ℃ in temperature for 24 h.
      Temperature test ① (−62±2) ℃, (70±2) ℃ for 2 h each; ② No peeling, stripping, cracking or bubbling on the film layer after the test Keep the test piece under (−62±2) ℃ and (70±2) ℃ for 2 h each, and place it under room temperature (16-32 ℃) (temperature change in the test chamber no faster than 2 ℃ /min), for test of adhesion
    Tools

    Get Citation

    Copy Citation Text

    Pengquan Zhang, Jiaqi Chen, Yijun Shi. Development of the aluminum substrate reflective film in the off-axis three-mirror optical system[J]. Infrared and Laser Engineering, 2022, 51(9): 20210900

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: Materials & Thin films

    Received: Nov. 25, 2021

    Accepted: Dec. 25, 2021

    Published Online: Jan. 6, 2023

    The Author Email:

    DOI:10.3788/IRLA20210900

    Topics