Bulletin of the Chinese Ceramic Society, Volume. 41, Issue 4, 1195(2022)
Glass Corrosion Resistance of Fused-Cast 41#AZS Material Containing Y2O3
[5] [5] FLEISCHMANN B. Fused cast AZS refractory materials: structure and structural changes during application[J]. Refractories World Forum, 2010, 2(2): 63.
[7] [7] STUBICAN V S, HINK R C, RAY S P. Phase equilibria and ordering in the system ZrO2-Y2O3[J]. Journal of the American Ceramic Society, 1978, 61(1/2): 17-21.
[9] [9] EVANS G. Fusion cast refractories for the glass industry[J]. Glass Technology, 2005, 46: 355-363.
[10] [10] PENA P, CRIADO E, BAKALI J J, et al. Dynamic corrosion of Al2O3-ZrO2-SiO2 and Cr2O3-containing refractories by molten frits. Part II: microstructural study[J]. Journal of the European Ceramic Society, 2011, 31(5): 705-714.
[11] [11] LI K M, SHI X Y, XUE F, et al. Static corrosion rates of fused-cast AZS refractory materials by molten glass[J]. Journal of the Chinese Ceramic Society, 2016, 3(4): 177-182.
Get Citation
Copy Citation Text
MAO Limin, LI Qingyuan, YANG Haiyun, ZENG Haijun, LIU Jiwang, QING Xiaobin, WANG Zhiyong, ZHU Wei, YANG Zhichao. Glass Corrosion Resistance of Fused-Cast 41#AZS Material Containing Y2O3[J]. Bulletin of the Chinese Ceramic Society, 2022, 41(4): 1195
Special Issue:
Received: Nov. 22, 2021
Accepted: --
Published Online: Aug. 3, 2022
The Author Email: Limin MAO (mlm@bjruitai.com)
CSTR:32186.14.