Bulletin of the Chinese Ceramic Society, Volume. 44, Issue 1, 31(2025)
Sulfate Corrosion Behavior in Solution Fully Soaked Magnesium Potassium Phosphate Cement Slurry
[3] [3] WAGH A S. Chemically bonded phosphate ceramics: twenty-first century materials with diverse applications[M]. 2nd ed. Amsterdam: Elsevier, 2016.
[6] [6] QIN J H, QIAN J S, YOU C, et al. Bond behavior and interfacial micro-characteristics of magnesium phosphate cement onto old concrete substrate[J]. Construction and Building Materials, 2018, 167: 166-176.
[7] [7] FENG H, SHEIKH M N, HADI M N S, et al. Interface bond performance of steel fibre embedded in magnesium phosphate cementitious composite[J]. Construction and Building Materials, 2018, 185: 648-660.
[9] [9] DING Z, LI Y Y, XU M R, et al. Electrochemical properties of aluminum tripolyphosphate modified chemically bonded phosphate ceramic anticorrosion coating[J]. Construction and Building Materials, 2020, 251: 118874.
[10] [10] CHONG L L, YANG J M, XU Z Z, et al. Freezing and thawing resistance of MKPC paste under different corrosion solutions[J]. Construction and Building Materials, 2019, 212: 663-674.
[12] [12] LI Y, SHI T F, LI J Q. Effects of fly ash and quartz sand on water-resistance and salt-resistance of magnesium phosphate cement[J]. Construction and Building Materials, 2016, 105: 384-390.
[13] [13] SHI J, ZHAO J G, CHEN H, et al. Sulfuric acid-resistance performances of magnesium phosphate cements: macro-properties, mineralogy and microstructure evolutions[J]. Cement and Concrete Research, 2022, 157: 106830.
[14] [14] ZOU D J, QIN S S, LIU T J, et al. Experimental and numerical study of the effects of solution concentration and temperature on concrete under external sulfate attack[J]. Cement and Concrete Research, 2021, 139: 106284.
[15] [15] ASTM International. Standard test method for length change of hydraulic-cement mortars exposed to a sulfate solution: ASTM C1012—04[S]. Pennsylvania, United States: ASTM International, 2010.
[18] [18] ASTM International. Standard test method for potential expansion of Portland-cement mortars exposed to sulfate: ASTM C452—21[S]. Pennsylvania, United States: ASTM International, 2010.
[21] [21] HOU Y Y, LI L, LI T, et al. Water-immersion stability of self-compacting potassium magnesium phosphate cement paste[J]. Materials, 2023, 16(6): 2183.
[22] [22] TUMIDAJSKI P J, CHAN G W, PHILIPOSE K E. An effective diffusivity for sulfate transport into concrete[J]. Cement and Concrete Research, 1995, 25(6): 1159-1163.
Get Citation
Copy Citation Text
HOU Yuying, YANG Jianming, XU Xiaohui, HU Xuexin, CHEN Weiliang, HU Xiamin, JIANG Dequan, XIONG Caiqiang, LI Tao. Sulfate Corrosion Behavior in Solution Fully Soaked Magnesium Potassium Phosphate Cement Slurry[J]. Bulletin of the Chinese Ceramic Society, 2025, 44(1): 31
Category:
Received: Aug. 5, 2024
Accepted: Feb. 18, 2025
Published Online: Feb. 18, 2025
The Author Email: Jianming YANG (yjm_kk@163.com)