Bulletin of the Chinese Ceramic Society, Volume. 43, Issue 10, 3772(2024)

Research Progress of Mechanism and Process of Thermal Debinding in 3D-Printed Ceramic Green Body

LUO Huangyang1... YANG Xianfeng1,*, LIU Ziyu1, LIU Peng1, XU Xiewen1 and XIE Zhipeng2 |Show fewer author(s)
Author Affiliations
  • 1School of Materials Science and Engineering, Changsha University of Science & Technology, Changsha 410004, China
  • 2State Key Laboratory of New Ceramic and Fine Processing, School of Materials Science and Engineering, Tsinghua University, Beijing 100083, China
  • show less
    References(105)

    [1] [1] CHEN Z W, LI Z Y, LI J J, et al. 3D printing of ceramics: a review[J]. Journal of the European Ceramic Society, 2019, 39(4): 661-687.

    [2] [2] LI Q L, QIU Y X, HOU W Q, et al. Slurry flow characteristics control of 3D printed ceramic core layered structure: experiment and simulation[J]. Journal of Materials Science & Technology, 2023, 164: 215-228.

    [3] [3] NIKOLINA K, SHENG L, KHAMIS E. Effect of the preparation techniques of photopolymerizable ceramic slurry and printing parameters on the accuracy of 3D printed lattice structures[J]. Journal of the European Ceramic Society, 2021, 41(15): 7734-7743.

    [4] [4] RANE K, PETR S, STRANO M. Evolution of porosity and geometrical quality through the ceramic extrusion additive manufacturing process stages[J]. Additive Manufacturing, 2020, 32: 101038.

    [6] [6] KRYACHEK V M. Injection moulding (review)[J]. Powder Metallurgy and Metal Ceramics, 2004, 43(7): 336-348.

    [7] [7] SUN J X, BINNER J, BAI J M. 3D printing of zirconia via digital light processing: optimization of slurry and debinding process[J]. Journal of the European Ceramic Society, 2020, 40(15): 5837-5844.

    [8] [8] TRAVITZKY N, BONET A, DERMEIK B, et al. Additive manufacturing of ceramic-based materials[J]. Advanced Engineering Materials, 2014, 16(6): 729-754.

    [9] [9] WU X Q, TENG J C, JI X X, et al. Research progress of the defects and innovations of ceramic vat photopolymerization[J]. Additive Manufacturing, 2023, 65: 103441.

    [10] [10] ZHANG K Q, MENG Q Y, QU Z L, et al. A review of defects in vat photopolymerization additive-manufactured ceramics: characterization, control, and challenges[J]. Journal of the European Ceramic Society, 2024, 44(3): 1361-1384.

    [11] [11] HOFER A K, RABITSCH J, JUTRZENKA-TRZEBIATOWSKA D, et al. Effect of binder system on the thermophysical properties of 3D-printed zirconia ceramics[J]. International Journal of Applied Ceramic Technology, 2022, 19(1): 174-180.

    [12] [12] ZAKERI S, VIPPOLA M, LEVNEN E. A comprehensive review of the photopolymerization of ceramic resins used in stereolithography[J]. Additive Manufacturing, 2020, 35: 101177.

    [13] [13] TAN L J, ZHU W, ZHOU K. Recent progress on polymer materials for additive manufacturing[J]. Advanced Functional Materials, 2020, 30(43): 2003062.

    [14] [14] LIM I Y, TING C H, NG C K, et al. 3D printing of high solid loading zirconia feedstock via screw-based material extrusion[J]. Ceramics International, 2023, 49(15): 24852-24860.

    [15] [15] HE Q L, JIANG J, YANG X F, et al. Additive manufacturing of dense zirconia ceramics by fused deposition modeling via screw extrusion[J]. Journal of the European Ceramic Society, 2021, 41(1): 1033-1040.

    [16] [16] SARRAF F, HADIAN A, CHURAKOV S V, et al. EVA-PVA binder system for polymer derived mullite made by material extrusion based additive manufacturing[J]. Journal of the European Ceramic Society, 2023, 43(2): 530-541.

    [17] [17] LI S, LI Y F, WANG Q W, et al. Fabrication of 3D-SiC/aluminum alloy interpenetrating composites by DIW and pressureless infiltration[J]. Ceramics International, 2021, 47(17): 24340-24347.

    [20] [20] LI H, ZHANG H, CHANG A, et al. A novel core-shell structure NTC ceramic with high stability fabricating by an in-situ ink-jet printing method[J]. Journal of the European Ceramic Society, 2021, 41(7): 4167-4174.

    [21] [21] LEE J H, KWEON J W, CHO W S, et al. Formulation and characterization of black ceramic ink for a digital ink-jet printing[J]. Ceramics International, 2018, 44(12): 14151-14157.

    [22] [22] QIN W, WANG K, ZHANG Y. Preparation of submicron CdSxSe1-x@ZrSiO4 inclusion pigment and its application in ink-jet printing[J]. Journal of the European Ceramic Society, 2021, 41(15): 7878-7885.

    [23] [23] PAN Z, WANG Y, HUANG H, et al. Recent development on preparation of ceramic inks in ink-jet printing[J]. Ceramics International, 2015, 41(10, Part A): 12515-12528.

    [24] [24] FIELDING G A, BANDYOPADHYAY A, BOSE S. Effects of silica and zinc oxide doping on mechanical and biological properties of 3D printed tricalcium phosphate tissue engineering scaffolds[J]. Dental Materials: Official Publication of the Academy of Dental Materials, 2012, 28(2): 113-122.

    [25] [25] NAN B Y, YIN X W, ZHANG L T, et al. Three-dimensional printing of Ti3SiC2-based ceramics[J]. Journal of the American Ceramic Society, 2011, 94(4): 969-972.

    [26] [26] SHAHZAD K, DECKERS J, KRUTH J P, et al. Additive manufacturing of alumina parts by indirect selective laser sintering and post processing[J]. Journal of Materials Processing Technology, 2013, 213(9): 1484-1494.

    [27] [27] LU D C, CHENG S, ZHANG L W, et al. Effect of holding time on SiC whiskers growth of SiCw/SiC composites based on SLS technology and their mechanical properties[J]. Ceramics International, 2022, 48(22): 33019-33027.

    [28] [28] KHAZAALAH T H, MUSTAFA I S, ALORAINI D A, et al. Investigation of optical properties and radioactive attenuation parameters of doped tungsten oxide soda lime silica SLS waste glass[J]. Journal of Materials Research and Technology, 2022, 19: 3355-3365.

    [29] [29] LU D C, ZHANG L W, CHENG S, et al. Microstructure control of SiCw/SiC composites based on SLS technology[J]. Journal of the European Ceramic Society, 2022, 42(9): 3747-3758.

    [30] [30] DENG K X, WU H H, LI Y, et al. Porous NFG/SiCnw composites fabricated by SLS for structural load-bearing and functionally integrated electromagnetic absorption[J]. Ceramics International, 2023, 49(17): 28547-28559.

    [31] [31] LEI J C, ZHANG Q R, WANG Y H, et al. Direct laser melting of Al2O3 ceramic paste for application in ceramic additive manufacturing[J]. Ceramics International, 2022, 48(10): 14273-14280.

    [32] [32] SU H, JIANG H, ZHANG Z, et al. Microstructure and mechanical properties of ZrB2-SiC eutectic composite ceramic fabricated by laser surface zone-melting: the effect of laser power and scanning speed[J]. Journal of the European Ceramic Society, 2023, 43(14): 5822-5829.

    [34] [34] DING G J, HE R J, ZHANG K Q, et al. Dispersion and stability of SiC ceramic slurry for stereolithography[J]. Ceramics International, 2020, 46(4): 4720-4729.

    [35] [35] XU X H, ZHOU S X, WU J F, et al. Relationship between the adhesion properties of UV-curable alumina suspensions and the functionalities and structures of UV-curable acrylate monomers for DLP-based ceramic stereolithography[J]. Ceramics International, 2021, 47(23): 32699-32709.

    [36] [36] LIU S, MO L N, BI G Y, et al. DLP 3D printing porous -tricalcium phosphate scaffold by the use of acrylate/ceramic composite slurry[J]. Ceramics International, 2021, 47(15): 21108-21116.

    [37] [37] WANG H H, HUANG Z Y, LI J, et al. DLP 3D printing of high-performance epoxy resin via dual curing[C]//2021 3rd International Academic Exchange Conference on Science and Technology Innovation (IAECST). Guangzhou, China. IEEE, 2021: 1172-1176.

    [38] [38] SANTOLIQUIDO O, CAMEROTA F, ORTONA A. The influence of topology on DLP 3D printing, debinding and sintering of ceramic periodic architectures designed to replace bulky components[J]. Open Ceramics, 2021, 5: 100059.

    [40] [40] KRONGAUZ V V. Crosslink density dependence of polymer degradation kinetics: photocrosslinked acrylates[J]. Thermochimica Acta, 2010, 503: 70-84.

    [41] [41] LEWIS J A. Binder removal from ceramics[J]. Annual Review of Materials Science, 1997, 27: 147-173.

    [42] [42] ZHANG D W, PENG E, BORAYEK R, et al. Controllable ceramic green-body configuration for complex ceramic architectures with fine features[J]. Advanced Functional Materials, 2019, 29(12): 1807082.

    [43] [43] KIM J, GAL C W, CHOI Y J, et al. Effect of non-reactive diluent on defect-free debinding process of 3D printed ceramics[J]. Additive Manufacturing, 2023, 67: 103475.

    [44] [44] WANG K, QIU M B, JIAO C, et al. Study on defect-free debinding green body of ceramic formed by DLP technology[J]. Ceramics International, 2020, 46(2): 2438-2446.

    [45] [45] MICLETTE O, CT R, DEMERS V, et al. Material extrusion additive manufacturing of low-viscosity metallic feedstocks: performances of the plunger-based approach[J]. Additive Manufacturing, 2022, 60: 103252.

    [46] [46] MCNULTY T F, MOHAMMADI F, BANDYOPADHYAY A, et al. Development of a binder formulation for fused deposition of ceramics[J]. Rapid Prototyping Journal, 1998, 4(4): 144-150.

    [47] [47] JAFARI M A, HAN W, MOHAMMADI F, et al. A novel system for fused deposition of advanced multiple ceramics[J]. Rapid Prototyping Journal, 2000, 6(3): 161-175.

    [48] [48] CLEMENS F, SCHULZ J, GORJAN L, et al. Debinding and sintering of dense ceramic structures made with fused deposition modeling[M]//Industrializing Additive Manufacturing. Cham: Springer International Publishing, 2020: 293-303.

    [49] [49] WAGNER M A, HADIAN A, SEBASTIAN T, et al. Fused filament fabrication of stainless steel structure: from binder development to sintered properties[J]. Additive Manufacturing, 2022, 49: 102472.

    [50] [50] LIU D M, TSENG W J. Binder removal from injection moulded zirconia ceramics[J]. Ceramics International, 1999, 25(6): 529-534.

    [51] [51] LI J, ZHANG C F, YIN R M, et al. Thermal debinding behavior of a low-toxic DMAA polymer for gelcast ceramic parts based on TG-FTIR and kinetic modeling[J]. RSC Advances, 2019, 9(15): 8415-8425.

    [52] [52] XIE H H, JIANG J, YANG X F, et al. Theory and practice of rapid and safe thermal debinding in ceramic injection molding[J]. International Journal of Applied Ceramic Technology, 2020, 17(3): 1098-1107.

    [53] [53] ZHANG L, HUANG J Y, XIAO Z H, et al. Effects of debinding condition on microstructure and densification of alumina ceramics shaped with photopolymerization-based additive manufacturing technology[J]. Ceramics International, 2022, 48(10): 14026-14038.

    [54] [54] CUI M M, WANG T, ZHAO Y, et al. Research on crack mechanism and kinetic model of alumina ceramic in the degreasing stage based on stereolithography[J]. International Journal of Applied Ceramic Technology, 2023, 20(6): 3419-3435.

    [55] [55] YAN X K, WANG C, XIONG W, et al. Thermal debinding mass transfer mechanism and dynamics of copper green parts fabricated by an innovative 3D printing method[J]. RSC Advances, 2018, 8(19): 10355-10360.

    [56] [56] SALEHI M, CLEMENS F, GRAULE T, et al. Kinetic analysis of the polymer burnout in ceramic thermoplastic processing of the YSZ thin electrolyte structures using model free method[J]. Applied energy, 2012, 95: 147-155.

    [57] [57] SHI Z, GUO Z X, SONG J H. A diffusion-controlled kinetic model for binder burnout in a powder compact[J]. Acta Materialia, 2002, 50(8): 1937-1950.

    [58] [58] CHEN Q H, ZOU B, LAI Q G, et al. A study on biosafety of HAP ceramic prepared by SLA-3D printing technology directly[J]. Journal of the Mechanical Behavior of Biomedical Materials, 2019, 98: 327-335.

    [59] [59] BOLGER J C. Acid base interactions between oxide surfaces and polar organic compounds[M]//Adhesion Aspects of Polymeric Coatings. Boston, MA: Springer US, 1983: 3-18.

    [62] [62] HOWARD K E, LAKEMAN C D E, PAYNE D A. Surface chemistry of various poly(vinyl butyral) polymers adsorbed onto alumina[J]. Journal of the American Ceramic Society, 1990, 73(8): 2543-2546.

    [63] [63] HRDINA K E, HALLORAN J W, OLIVEIRA A, et al. Chemistry of removal of ethylene vinyl acetate binders[J]. Journal of Materials Science, 1998, 33(11): 2795-2803.

    [64] [64] KNAPP A M, HALLORAN J W. Binder removal from ceramic-filled thermoplastic blends[J]. Journal of the American Ceramic Society, 2006, 89(9): 2776-2781.

    [65] [65] ZUBRZYCKA P, RADECKA M, GRAULE T, et al. Debinding of additively manufactured parts from spinel powders with particle sizes below 200nm[J]. Ceramics International, 2023, 49(7): 11355-11367.

    [66] [66] LI Y M, JIANG F, ZHAO L G, et al. Critical thickness in binder removal process for injection molded compacts[J]. Materials Science and Engineering: A, 2003, 362(1/2): 292-299.

    [67] [67] GENTRY S P, HALLORAN J W. Depth and width of cured lines in photopolymerizable ceramic suspensions[J]. Journal of the European Ceramic Society, 2013, 33(10): 1981-1988.

    [68] [68] AGGARWAL G, PARK S J, SMID I, et al. Master decomposition curve for binders used in powder injection molding[J]. Metallurgical and Materials Transactions A, 2007, 38(3): 606-614.

    [69] [69] SHEN Y R, SUN Y, JIN B C, et al. Effect of debinding and sintering profile on the optical properties of DLP-3D printed YAG transparent ceramic[J]. Ceramics International, 2022, 48(15): 21134-21140.

    [70] [70] LI H, LIU Y S, LIU Y S, et al. Effect of debinding temperature under an argon atmosphere on the microstructure and properties of 3D-printed alumina ceramics[J]. Materials Characterization, 2020, 168: 110548.

    [71] [71] LI H, LIU Y S, LIU Y S, et al. Microstructure and properties of 3D-printed alumina ceramics with different heating rates in vacuum debinding[J]. Rare Metals, 2020, 39(5): 577-588.

    [72] [72] ZHOU M P, LIU W, WU H D, et al. Preparation of a defect-free alumina cutting tool via additive manufacturing based on stereolithography-optimization of the drying and debinding processes[J]. Ceramics International, 2016, 42(10): 11598-11602.

    [74] [74] MCALEER E G, ALAZZAWI M K, HWANG C, et al. Binder removal from ceramic stereolithography green bodies: a neutron imaging and thermal analysis study[J]. Journal of the American Ceramic Society, 2023, 106(7): 4399-4410.

    [75] [75] LI H, LIU Y S, LIU Y S, et al. Influence of debinding holding time on mechanical properties of 3D-printed alumina ceramic cores[J]. Ceramics International, 2021, 47(4): 4884-4894.

    [76] [76] PRIEL Z, SILBERBERG A. The thickness of adsorbed polymer layers at a liquid-solid interface as a function of bulk concentration[J]. Journal of Polymer Science: Polymer Physics Edition, 1978, 16(11): 1917-1925.

    [77] [77] KIM I, KIM S, ANDREU A, et al. Influence of dispersant concentration toward enhancing printing precision and surface quality of vat photopolymerization 3D printed ceramics[J]. Additive Manufacturing, 2022, 52: 102659.

    [78] [78] HAN Z Q, LIU S H, QIU K, et al. The enhanced ZrO2 produced by DLP via a reliable plasticizer and its dental application[J]. Journal of the Mechanical Behavior of Biomedical Materials, 2023, 141: 105751.

    [79] [79] CIMA M J, LEWIS J A, DEVOE A D. Binder distribution in ceramic greenware during thermolysis[J]. Journal of the American Ceramic Society, 1989, 72(7): 1192-1199.

    [80] [80] BAE C J, HALLORAN J W. Influence of residual monomer on cracking in ceramics fabricated by stereolithography[J]. International Journal of Applied Ceramic Technology, 2011, 8(6): 1289-1295.

    [81] [81] YIN Y H, WANG J, HUANG Q Q, et al. Influence of debinding parameter and nano-ZrO2 particles on the silica-based ceramic cores fabricated by stereolithography-based additive manufacturing[J]. Ceramics International, 2023, 49(12): 20878-20889.

    [82] [82] GERMAN R M. Theory of thermal debinding[J]. International Journal of Powder Metallurgy, 1987, 23: 237-245.

    [83] [83] ANGERMANN H H, YANG F K, VAN DER BIEST O. Removal of low molecular weight components during thermal debinding of powder compacts[J]. Journal of Materials Science, 1992, 27(9): 2534-2538.

    [85] [85] LEWIS J A, GALLER M A, BENTZ D P. Computer simulations of binder removal from 2-D and 3-D model particulate bodies[J]. Journal of the American Ceramic Society, 1996, 79(5): 1377-1388.

    [86] [86] GERMAN R M. Injection molding of metals and ceramics[J]. Powder Metallurgy, 1997, 42: 157-160.

    [87] [87] WU H D, CHENG Y L, LIU W, et al. Effect of the particle size and the debinding process on the density of alumina ceramics fabricated by 3D printing based on stereolithography[J]. Ceramics International, 2016, 42(15): 17290-17294.

    [88] [88] XING H Y, ZOU B, LIU X Y, et al. Effect of particle size distribution on the preparation of ZTA ceramic paste applying for stereolithography 3D printing[J]. Powder Technology, 2020, 359: 314-322.

    [89] [89] MATAR S A, EVANS J R G, EDIRISINGHE M J, et al. The effect of porosity development on the removal of organic vehicle from ceramic or metal moldings[J]. Journal of Materials Research, 1993, 8(3): 617-625.

    [90] [90] LI J, HUANG J D, YIN R M. Multistage kinetic analysis of DMAA/MBAM polymer removal from gelcast ceramic parts using a multi-stage parallel reaction model and model-free method[J]. RSC Advances, 2019, 9(47): 27305-27317.

    [91] [91] KHOONG L E, LAM Y C, CHAI J C, et al. Modeling of mass transfers in a porous green compact with two-component binder during thermal debinding[J]. Chemical Engineering Science, 2009, 64(12): 2837-2850.

    [92] [92] LI J, ZHANG C F, YIN R M, et al. DAEM kinetics analysis and finite element simulation of thermal debinding process for a gelcast SiAlON green body[J]. Ceramics International, 2019, 45(7): 8166-8174.

    [93] [93] CHICONE C, LOMBARDO S J, RETZLOFF D G. Modeling, approximation, and time optimal temperature control for binder removal from ceramics[J]. Discrete & Continuous Dynamical Systems-B, 2022, 27(1): 103.

    [94] [94] SONG J H, EVANS J R G, EDIRISINGHE M J, et al. Optimization of heating schedules in pyrolytic binder removal from ceramic moldings[J]. Journal of Materials Research, 2000, 15(2): 449-457.

    [95] [95] LAM Y C, YU S C M, TAM K C, et al. Simulation of polymer removal from a powder injection molding compact by thermal debinding[J]. Metallurgical and Materials Transactions A, 2000, 31(10): 2597-2606.

    [96] [96] GORJAN L, LUSIOLA T, SCHARF D, et al. Kinetics and equilibrium of eco-debinding of PZT ceramics shaped by thermoplastic extrusion[J]. Journal of the European Ceramic Society, 2017, 37(16): 5273-5280.

    [97] [97] ESAN O J, HANSEN C J, PETERSON A M. Multiphysics and geometry-based modeling of incorporating mass transport networks in ceramic green bodies to improve thermal debinding[J]. Ceramics International, 2024, 50(6): 9789-9800.

    [98] [98] ZHOU S X, LIU G Z, WANG C S, et al. Thermal debinding for stereolithography additive manufacturing of advanced ceramic parts: a comprehensive review[J]. Materials & Design, 2024, 238: 112632.

    [99] [99] ENNETI R K, PARK S J, GERMAN R M, et al. Review: thermal debinding process in particulate materials processing[J]. Materials and Manufacturing Processes, 2012, 27(2): 103-118.

    [100] [100] JOHANSSON E, LIDSTRM O, JOHANSSON J, et al. Influence of resin composition on the defect formation in alumina manufactured by stereolithography[J]. Materials, 2017, 10(2): 138.

    [101] [101] NIU F R, YANG X L, LI Y B, et al. Fused deposition modeling of Si3N4 ceramics: a cost-effective 3D-printing route for dense and high performance non-oxide ceramic materials[J]. Journal of the European Ceramic Society, 2022, 42(15): 7369-7376.

    [102] [102] XING H Y, ZOU B, LI S S, et al. Study on surface quality, precision and mechanical properties of 3D printed ZrO2 ceramic components by laser scanning stereolithography[J]. Ceramics International, 2017, 43(18): 16340-16347.

    [103] [103] LI H, LIU Y S, LIU Y S, et al. Influence of vacuum debinding temperature on microstructure and mechanical properties of three-dimensional-printed alumina via stereolithography[J]. 3D Printing and Additive Manufacturing, 2020, 7(1): 8-18.

    [104] [104] SCHERER G W. Theory of drying[J]. Journal of the American Ceramic Society, 1990, 73(1): 3-14.

    [105] [105] ZHANG K Q, MENG Q Y, ZHANG X Q, et al. Quantitative characterization of defects in stereolithographic additive manufactured ceramic using X-ray computed tomography[J]. Journal of Materials Science & Technology, 2022, 118: 144-157.

    [106] [106] HSIANG H I, LEE C Y, CHEN C C, et al. Polycrystalline alumina ceramic fabrication using digital stereolithographic light process[J]. Ceramics International, 2021, 47(23): 33815-33826.

    [107] [107] YANG S D, ZHANG R J, QU X H. X-ray tomographic analysis of powder-binder separation in SiC green body[J]. Journal of the European Ceramic Society, 2013, 33(15/16): 2935-2941.

    [108] [108] LU P K, LANNUTTI J J. Effect of density gradients on dimensional tolerance during binder removal[J]. Journal of the American Ceramic Society, 2000, 83(10): 2536-2542.

    [109] [109] STROBL M, MANKE I, KARDJILOV N, et al. Advances in neutron radiography and tomography[J]. Journal of Physics D: Applied Physics, 2009, 42(24): 243001.

    [110] [110] ZHANG K Q, MENG Q Y, CAI N J, et al. Effects of solid loading on stereolithographic additive manufactured ZrO2 ceramic: a quantitative defect study by X-ray computed tomography[J]. Ceramics International, 2021, 47(17): 24353-24359.

    [111] [111] ZHANG K, MENG Q, ZHANG X, et al. Roles of solid loading in stereolithography additive manufacturing of ZrO2 ceramic[J]. International Journal of Refractory Metals and Hard Materials, 2021, 99: 105604.

    [112] [112] WANG X Y, DUAN W Y, CHEN Z H, et al. Uniform rate debinding for Si3N4 vat photopolymerization 3D printing green parts using a specific-stage stepwise heating process[J]. Additive Manufacturing, 2024, 84: 104119.

    [113] [113] ORTEGA VARELA DE SEIJAS M, BARDENHAGEN A, PAMBAGUIAN L, et al. Laser debinding of parts produced through material extrusion additive manufacturing[J]. Journal of Manufacturing Processes, 2023, 88: 1-11.

    [114] [114] CANILLAS M, JEAN F, THUAULT A, et al. Microwave-assisted debinding of Al2O3 parts printed by stereolithography[J]. Ceramics International, 2023, 49(11): 18343-18352.

    Tools

    Get Citation

    Copy Citation Text

    LUO Huangyang, YANG Xianfeng, LIU Ziyu, LIU Peng, XU Xiewen, XIE Zhipeng. Research Progress of Mechanism and Process of Thermal Debinding in 3D-Printed Ceramic Green Body[J]. Bulletin of the Chinese Ceramic Society, 2024, 43(10): 3772

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category:

    Received: Apr. 9, 2024

    Accepted: Jan. 17, 2025

    Published Online: Jan. 17, 2025

    The Author Email: Xianfeng YANG (yangxfcsust@csust.edu.cn)

    DOI:

    CSTR:32186.14.

    Topics