Journal of the Chinese Ceramic Society, Volume. 51, Issue 12, 3144(2023)
Textured SiAlON Ceramic with Centripetal Grain Alignment
A textured SiAlON ceramic with a centripetal grain alignment was obtained via sinter-forging through outer diameter strain ring compression using spark plasma heating. The microstructure, texturing degree and anisotropy of mechanical properties of the ceramic were investigated. The results show that the c-axis (i.e., long axis) of the rod-like SiAlON grains is parallel to the radial direction of the cylindrical sample, forming a centripetal grain alignment. The average included angle between the c-axis and radial direction is 19.2° and 9.9° on the plane perpendicular to pressing direction and parallel to radial direction, respectively. The degree of centripetal texture is 0.79. The hardness on the plane perpendicular to pressing direction is 12% greater than that on the plane perpendicular to radial section, reaching 17.85 GPa. The flexural strength with fracture plane perpendicular to radial section is 57% greater than that with fracture direction parallel to radial direction, which is 1 341 MPa. The fracture toughness with crack propagation perpendicular to radial section is 75% higher than that with crack direction parallel to radial direction, which is 6.27 MPa·m1/2.
Get Citation
Copy Citation Text
XIAO Shuiqing, TAN Dawang, LI Wei, GUO Weiming, LIN Huatay. Textured SiAlON Ceramic with Centripetal Grain Alignment[J]. Journal of the Chinese Ceramic Society, 2023, 51(12): 3144
Received: Jun. 13, 2023
Accepted: --
Published Online: Jan. 19, 2024
The Author Email:
CSTR:32186.14.