Bulletin of the Chinese Ceramic Society, Volume. 43, Issue 3, 1133(2024)

Structural and properties Evolution of Al2O3-SiO2 Refractories under Simulated Hydrogen-Based Shaft Furnace Condition

XIE Fubo1...2, LI Yawei1,2,*, LIAO Ning1,2, SHI Chenglong3, CAI Guoqing3 and QIN Jiantao3 |Show fewer author(s)
Author Affiliations
  • 1[in Chinese]
  • 2[in Chinese]
  • 3[in Chinese]
  • show less
    References(24)

    [1] [1] XIONG L. Research on development status of metallurgical engineering technology in low-carbon economy[J]. China Metal Bulletin, 2022(22): 1-3 (in Chinese).

    [2] [2] GUO X Y, CHEN Y L, TIAN Q H, et al. Research progress on hydrogen metallurgy theory and method[J]. The Chinese Journal of Nonferrous Metals, 2021, 31(7): 1891-1906 (in Chinese).

    [3] [3] LIU Z G, HUI S X. Research progress of hydrogen metallurgy principle and industrial application[J]. China Metal Bulletin, 2021(9): 5-6 (in Chinese).

    [4] [4] WANG R R, ZHAO Y Q, BABICH A, et al. Hydrogen direct reduction (H-DR) in steel industry: an overview of challenges and opportunities[J]. Journal of Cleaner Production, 2021, 329: 129797.

    [5] [5] LIU Z J, LU S F, WANG Y Z, et al. Study on optimization of reduction temperature of hydrogen-based shaft furnace: numerical simulation and multi-criteria evaluation[J]. International Journal of Hydrogen Energy, 2023, 48(42): 16132-16142.

    [6] [6] TANG J, CHU M S, LI F, et al. Development and progress on hydrogen metallurgy[J]. International Journal of Minerals, Metallurgy and Materials, 2020, 27(6): 713-723.

    [7] [7] BAI M H, LONG H, REN S B, et al. Reduction behavior and kinetics of iron ore pellets under H2-N2 atmosphere[J]. ISIJ International, 2018, 58(6): 1034-1041.

    [8] [8] NAGASAKA T, HINO M, BAN-YA S. Interfacial kinetics of hydrogen with liquid slag containing iron oxide[J]. Metallurgical and Materials Transactions B, 2000, 31(5): 945-955.

    [9] [9] FANG J. Non-blast furnace ironmaking technology and theory[M]. Beijing: Metallurgical Industry Press, 2002: 1-62 (in Chinese).

    [10] [10] GE J L. Study on the relationship between furnace behavior and furnace type in gas-based direct reduction shaft furnace[D].Qinhuangdao: Yanshan University, 2014 (in Chinese).

    [11] [11] ZHOU Y, ZHOU H J, XU C M. Exploration of hydrogen sources for the low-carbon and green production in the steel industry in China[J]. Chemical Industry and Engineering Progress, 2022, 41(2): 1073-1077 (in Chinese).

    [12] [12] YU G H, CUI J W, ZHAO F, et al. Service environment simulation and design of refractory for hydrogen-based shaft furnace[J]. Journal of the Chinese Ceramic Society, 2023, 51(3): 619-627 (in Chinese).

    [13] [13] SANG S B, PU J, JIANG S P, et al. Prediction of H2 leak rate in mica-based seals of planar solid oxide fuel cells[J]. Journal of Power Sources, 2008, 182(1): 141-144.

    [14] [14] BONALDE A, HENRIQUEZ A, MANRIQUE M. Kinetic analysis of the iron oxide reduction using hydrogen-carbon monoxide mixtures as reducing agent[J]. ISIJ International, 2005, 45(9): 1255-1260.

    [15] [15] HAN X L, LIU J L. Application of refractory materials[M]. Beijing: Metallurgical Industry Press, 1986 (in Chinese).

    [16] [16] LI Y, CHEN L, HONG L, et al. Fabrication of porous silicon carbide ceramics at low temperature using aluminum dihydrogen phosphate as binder[J]. Journal of Alloys and Compounds, 2019, 785: 838-845.

    [17] [17] ROUSSEAU G, MONTAGNE L, MAR F O. Further insights on the thermal degradation of aluminum metaphosphate prepared from aluminum dihydrogen phosphate solution[J]. Journal of the European Ceramic Society, 2021, 41(9): 4970-4976.

    [18] [18] WANG Z F, MA S L, REN B, et al. Microstructural evolution of andalusite at elevated temperature and its potassium vapor attack resistance behavior[J]. Bulletin of the Chinese Ceramic Society, 2023, 42(3): 1106-1114 (in Chinese).

    [19] [19] LI L S, LIAO G H, XU G H. Effect of firing temperature and soaking time on mollitization of andalusite based refractory[J]. Bulletin of the Chinese Ceramic Society, 2007, 26(6): 1229-1232+1239 (in Chinese).

    [20] [20] MONDAL K, LORETHOVA H, HIPPO E, et al. Reduction of iron oxide in carbon monoxide atmosphere: reaction controlled kinetics[J]. Fuel Processing Technology, 2004, 86(1): 33-47.

    [21] [21] BONALDE A, HENRIQUEZ A, MANRIQUE M. Kinetic analysis of the iron oxide reduction using hydrogen-carbon monoxide mixtures as reducing agent[J]. ISIJ International, 2005, 45(9): 1255-1260.

    [22] [22] XU M W P, BROWN J J Jr. Mechanism of iron catalysis of carbon monoxide decomposition in refractories[J]. Journal of the American Ceramic Society, 1989, 72(1): 110-115.

    [23] [23] ASTM. Standard test method for disintegration of refractories in an atmosphere of carbon monoxide: C288-87[S]. PA: ASTM, 2014.

    [24] [24] British Standards Institution. Methods of testing refractory materials, general and textural properties, determination of resistance to carbon monoxide: BS 1902-3[S]. Britain: GB-BSI, 1988.

    Tools

    Get Citation

    Copy Citation Text

    XIE Fubo, LI Yawei, LIAO Ning, SHI Chenglong, CAI Guoqing, QIN Jiantao. Structural and properties Evolution of Al2O3-SiO2 Refractories under Simulated Hydrogen-Based Shaft Furnace Condition[J]. Bulletin of the Chinese Ceramic Society, 2024, 43(3): 1133

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category:

    Received: Sep. 19, 2023

    Accepted: --

    Published Online: Aug. 2, 2024

    The Author Email: Yawei LI (liyawei@wust.edu.cn)

    DOI:

    CSTR:32186.14.

    Topics