Bulletin of the Chinese Ceramic Society, Volume. 41, Issue 3, 884(2022)
Effects of Fly ash and Slag Particle Size Distributions on Microstructure and Chloride Ion Penetration Resistance of Concrete
[3] [3] BEHERA S K, MISHRA D P, SINGH P, et al. Utilization of mill tailings, fly ash and slag as mine paste backfill material: review and future perspective[J]. Construction and Building Materials, 2021, 309: 125120.
[5] [5] WANG X Y. Analysis of hydration kinetics and strength progress in cement-slag binary composites[J]. Journal of Building Engineering, 2021, 35: 101810.
[7] [7] FULLER W B, THOMPSON S E. The laws of proportioning concrete[J]. Transactions of the American Society of Civil Engineers, 1907, 59(2): 67-143.
[11] [11] CAO C, CHEUNG M M S. Non-uniform rust expansion for chloride-induced pitting corrosion in RC structures[J]. Construction and Building Materials, 2014, 51: 75-81.
[13] [13] ZHAO H, SUN W, WU X M, et al. The properties of the self-compacting concrete with fly ash and ground granulated blast furnace slag mineral admixtures[J]. Journal of Cleaner Production, 2015, 95: 66-74.
[14] [14] FAN J C, ZHU H G, SHI J, et al. Influence of slag content on the bond strength, chloride penetration resistance, and interface phase evolution of concrete repaired with alkali activated slag/fly ash[J]. Construction and Building Materials, 2020, 263: 120639.
[15] [15] ZARZUELA R, LUNA M, CARRASCOSA L M, et al. Producing C-S-H gel by reaction between silica oligomers and portlandite: a promising approach to repair cementitious materials[J]. Cement and Concrete Research, 2020, 130: 106008.
[17] [17] LI W T, YI Y L. Use of carbide slag from acetylene industry for activation of ground granulated blast-furnace slag[J]. Construction and Building Materials, 2020, 238: 117713.
[18] [18] PHOO-NGERNKHAM T, PHIANGPHIMAI C, INTARABUT D, et al. Low cost and sustainable repair material made from alkali-activated high-calcium fly ash with calcium carbide residue[J]. Construction and Building Materials, 2020, 247: 118543.
[19] [19] YI Y, LI C, LIU S, et al. Magnesium sulfate attack on clays stabilised by carbide slag- and magnesia-ground granulated blast furnace slag[J]. Géotechnique Letters, 2015, 5(4): 306-312.
[21] [21] DE AZEVEDO N H, DE MATOS P R, GLEIZE P J P, et al. Effect of thermal treatment of SiC nanowhiskers on rheological, hydration, mechanical and microstructure properties of Portland cement pastes[J]. Cement and Concrete Composites, 2021, 117: 103903.
[22] [22] CHEN X, LI J S, XUE Q, et al. Sludge biochar as a green additive in cement-based composites: mechanical properties and hydration kinetics[J]. Construction and Building Materials, 2020, 262: 120723.
[23] [23] CHENG X J, SHI L, LIU Q Y, et al. Heat effects of pyrolysis of 15 acid washed coals in a DSC/TGA-MS system[J]. Fuel, 2020, 268: 117325.
[25] [25] GWON S, CHOI Y C, SHIN M. Effect of plant cellulose microfibers on hydration of cement composites[J]. Construction and Building Materials, 2021, 267: 121734.
Get Citation
Copy Citation Text
AN Qiang, PAN Huimin, WANG Shuai, ZHAO Qingxin. Effects of Fly ash and Slag Particle Size Distributions on Microstructure and Chloride Ion Penetration Resistance of Concrete[J]. Bulletin of the Chinese Ceramic Society, 2022, 41(3): 884