Journal of Inorganic Materials, Volume. 37, Issue 4, 436(2022)

Dentin Remineralization Induced by Micro-nano Bioactive Glass Spheres

Figures & Tables(12)
SEM (a1-c1), TEM (a2-c2) images and particle size distributions (a3-c3) of MNBGs
XRD patterns (a) and FT-IR spectra (b) of MNBGs
SEM images of the dentin surface without (a) and with (b) EDTA-etching, magnified photo of dentin tubules (insert in (b)), and photo of bioactive glass paste (c)
SEM images of demineralized dentin slices coating with different MNBGP
ATR-FTIR spectra of demineralized dentin surface before and after coating with MNBGP, and after rinsing with water
SEM images of the surfaces of demineralized dentin slices without (a) (control) and with treatment by MNBGP-1 (b), MNBGP-2 (c), and MNBGP-3 (d) after soaking in AS for 1 d (a1-d1), 7 d (a2-d2), 14 d (a3-d3) and 28 d (a4-d4)
SEM images of the longitudinal section of demineralized dentin samples without (a) (control) and with treatment by MNBGP-1 (b), MNBGP-2 (c), and MNBGP-3 (d) after soaking in AS for 1 d (a1-d1), 7 d (a2-d2), 14 d (a3-d3) and 28 d (a4-d4)
EDS analyses of the surface of demineralized dentin slices without (a) (control) and with treatment by MNBGP-1 (b), MNBGP-2 (c), and MNBGP-3 (d) after soaking in AS for 28 d
XRD patterns of the surface of intact dentin, demineralized dentin and slices without treatment (control) and being treated with MNBGP after being soaked in AS for 28 d
  • Table 1. Theoretical and measured chemical composition, reagent dosage of MNBGs with different particle sizes

    View table
    View in Article

    Table 1. Theoretical and measured chemical composition, reagent dosage of MNBGs with different particle sizes

    SampleSiO2 : CaO : P2O5 (molar ratio) DDA/gTEOS/mL
    TheoreticalMeasured
    MNBGs-180 : 16 : 487.637 : 12.363 : 038
    MNBGs-286.289 : 13.696 : 0.015616
    MNBGs-389.071 : 10.875 : 0.054624
  • Table 2. Chemical components (molar percent) and Ca/P ratio on the surface of dentin before and after EDTA etching

    View table
    View in Article

    Table 2. Chemical components (molar percent) and Ca/P ratio on the surface of dentin before and after EDTA etching

    SamplesC/%O/%Ca/%P/%Ca/P
    Without etching065.7720.2613.971.45
    With etching66.8232.990.050.140.35
  • Table 3. Chemical components ( molar percent) and Ca/P ratio in molar on the surface of remineralized dentin

    View table
    View in Article

    Table 3. Chemical components ( molar percent) and Ca/P ratio in molar on the surface of remineralized dentin

    SampleCa/%P/%Ca/P
    Control2.491.821.37
    MNBGP-116.6411.691.42
    MNBGP-218.3712.971.42
    MNBGP-36.166.121.01
Tools

Get Citation

Copy Citation Text

. Dentin Remineralization Induced by Micro-nano Bioactive Glass Spheres[J]. Journal of Inorganic Materials, 2022, 37(4): 436

Download Citation

EndNote(RIS)BibTexPlain Text
Save article for my favorites
Paper Information

Category: RESEARCH ARTICLE

Received: Mar. 12, 2021

Accepted: --

Published Online: Jan. 10, 2023

The Author Email:

DOI:10.15541/jim20210158

Topics