    In the present paper,different corrosions of three pieces of Chinese ancient lead glazed potteries from different burial circumstances were analyzed by using XRD,FTIR,EDXRF,RS etc,and the analyses indicate that the main crystalline phase of corrosion of HYT is cerussite (PbCO3),that of SYT is calcium-lead hydroxyapatite [Pb10-xCax(PO4)(OH)2(x<2.7)] and the yellow area of the erosion is attributed to a certain mount of iron oxide,that of TSC is the cerussite (PbCO3) and calcium-lead hydroxyapatite [Pb10-xCax(PO4)(OH)2(x<2.7)],and the brown-black area of the erosion product is the result of the existence of little mount of iron and carbon black.

    Tools

    Get Citation

    Copy Citation Text

    ZHU Tie-quan, WANG Chang-sui, MAO Zhen-wei, LI Li-xin, HUANG Hong. Identification of Different Corrosion Covering the Surface of Chinese Ancient Lead Glazed Potteries[J]. Spectroscopy and Spectral Analysis, 2010, 30(1): 266

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Received: Dec. 22, 2008

    Accepted: --

    Published Online: Jul. 13, 2010

    The Author Email: Tie-quan ZHU (zhutq@mail.ustc.edu.cn)

    DOI:10.3964/j.issn.1000-0593(2010)01-0266-04

    Topics