Acta Optica Sinica, Volume. 27, Issue 6, 1129(2007)

Laser Damage Characteristic of Third Harmonic Separator at 1064 nm

[in Chinese]1,2、*, [in Chinese]1, [in Chinese]1, [in Chinese]1, and [in Chinese]1
Author Affiliations
  • 1[in Chinese]
  • 2[in Chinese]
  • show less

    The two kinds of 3ω harmonic separator were prepared by electron beam evaporation with different materials. Laser induced damage threshold (LIDT) was measured at 1064 nm and the damage morphologies were mapped by Alpha-Step 500 meter. It was found that there are two different damage geometries: shallow denudation and deep crater. Shallow denudation in a certain range had same depth at different energy fluences, and material was removed from the top film layers. Deep crater had different depths caused by the combination of melting vaporization and fracture of inner defects of coatings, which was the main cause for decreased damage threshold.

    Tools

    Get Citation

    Copy Citation Text

    [in Chinese], [in Chinese], [in Chinese], [in Chinese], [in Chinese]. Laser Damage Characteristic of Third Harmonic Separator at 1064 nm[J]. Acta Optica Sinica, 2007, 27(6): 1129

    Download Citation

    EndNote(RIS)BibTexPlain Text
    Save article for my favorites
    Paper Information

    Category: Thin Films

    Received: Aug. 14, 2006

    Accepted: --

    Published Online: Jun. 8, 2007

    The Author Email: (cuiyun@siom.ac.cn)